Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0105 cm/cm | 0.0105 in/in | STN EN ISO 294-4 |
Plastcom PLASTAMID® 66 GF 35 TS 002 PA66 reinforced with glass fiber, heat stabilized PA66 for injection molding, reinforced with 35 % glass fiber, heat stabilized, used in automotive, engineering and electrical industry, eg. intake pipes, cylinder heads, induction coils, carrying pa.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 cm/cm | 0.0105 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 FRC 2 LS Polyamide 6, Halogen Free Flame Retardant, Light Stabilization FeaturesLongterm external use is possible because of the material stabilization with the light stabilizers on the HALS basis. Meets the flammability in accordance with the norm DIN 4102 - B1. PA 6.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 cm/cm | 0.0105 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 GF 35 Polyamide 66, 35% Glass Fiber FeaturesChemically reinforced with 35% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 cm/cm | 0.0105 in/in | LATI |
LATI LARPEEK 10 G/30 30% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0185 cm/cm | 0.0105 - 0.0185 in/in | Average value: 0.0131 cm/cm Grade Count:19 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 cm/cm | 0.0105 in/in | 60x60x2; 300°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.014 cm/cm | 0.0105 - 0.014 in/in | |
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latilub 66 Y/20 PA66, Aramid Fiber Reinforced Self-lubricating product based on Polyamide 66 (PA66). Aramid fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termo.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latilub 75/4-15ST G/30 PBT, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polybutylene Terephthalate (PBT). Silicone / PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latimass 66-04 D009 PBT Specific density compound based on Polybutylene Terephthalate (PBT). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latistat 62-06 K/10 PA6, 10% Carbon Fiber Reinforced Dissipative product based on Polyamide 6 (PA6). Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplasti.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 cm/cm @Thickness 2.00 mm |
0.0105 in/in @Thickness 0.0787 in |
TPE Method |
SCG Chemicals EL-Proâ„¢ P440J Polypropylene Injection Molding Key Characteristics:Excellent impact strengthSuitable for small to medium partsRecommended Applications:High impact and durable automotive, motorcycle and electrical appliance parts such as fan stan.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 cm/cm | 0.0105 in/in | Annealed; ISO 294-4 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 cm/cm | 0.0105 in/in | Annealed; ISO 294-4 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.0135 cm/cm | 0.0105 - 0.0135 in/in | |
LATI Latimass 52/11-04 D008 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 cm/cm | 0.0105 in/in | TD |
Aclo Accutech TPO TPO030T9V Paintable Grade Approved to Suzuki Spec Black B14257 |
|||
Linear Mold Shrinkage, Transverse | 0.0105 - 0.013 cm/cm | 0.0105 - 0.013 in/in | |
LATI Latamid 66 H2 G/25-V0KB4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Linear Mold Shrinkage, Transverse | 0.0105 cm/cm @Thickness 2.00 mm |
0.0105 in/in @Thickness 0.0787 in |
TPE Method |
SCG Chemicals EL-Pro™ P441JU Polypropylene Injection Molding Key Characteristics:Excellent impact strengthContains UV stabilizer and anti-static agentSuitable for small to medium partsRecommended Applications:High impact and durable automotive and electrical .. |