| Category | Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , TPO |
| Manufacturer | Aclo Compounders |
| Trade Name | Accutech |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Aclo Accutech TPO TPO030T9V Paintable Grade.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.965 g/cc | 0.0349 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | MD; ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.0105 cm/cm | 0.0105 in/in | TD |
| Melt Flow | 35 g/10 min | 35 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 85 | 85 | ASTM D785 |
| Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
| Elongation at Break | 100 % | 100 % | ASTM D638 |
| Tensile Modulus | 1.350 GPa | 195.8 ksi | ASTM D638 |
| Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
| Izod Impact, Notched | 0.534 J/cm @Temperature -30.0 °C |
1.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
| Heat Distortion | 210250 % | 210250 % | ASTM D790 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 67.0 µm/m-°C @Temperature 20.0 °C |
37.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 115 °C | 239 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C | 158 °F |