Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0025 cm/cm | 0.0025 in/in | LATI |
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 cm/cm | 0.0025 in/in | LATI |
LATI LATILUB 95-25GR CE/10 Polysulfone Base (PSU), 25% Graphite, 10% Special Mineral Filled Self Lubricating Plastic Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | Test Condition: 150x105x3; acc. ISO 2577 |
Ineos ABS Lustran® SAN GF20 Glass Fiber Reinforced |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 cm/cm | 0.0025 in/in | ISO 2577 |
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP HPC 1200 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 cm/cm | 0.0025 in/in | ISO 2577 |
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP HPC 1300 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Laticonther 62 GR/70 PA 6, 70% Graphite Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | |
LATI Laticonther 80 CPG/700 PPS, Glass Fiber Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Special filler. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0055 cm/cm | 0.0025 - 0.0055 in/in | |
LATI Laticonther 82 CP1/800 PA12 High thermal conductivity product based on Polyamide 12 (PA12). Special fillerAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Latigloss 57 G/60 F2 PPA, 60% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | |
LATI Latilub 87/28-15T K/20 PC, 20% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Latiohm 85-06 PD01 G/15 PES, 15% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyether Sulfone (PES). Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0025 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0025 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+PS LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0040 cm/cm @Time 86400 sec |
0.0025 - 0.0040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp GC006XXZ PSU LNP THERMOCOMP* GC006XXZ is a compound based on Polysulfone resin containing Carbon Fiber.This product is also known as Thermocomp* GC-1006.This data was supplied by SABIC-IP for the Americas region.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0076 cm/cm @Thickness 3.20 mm |
0.0025 - 0.0076 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP 30% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0076 cm/cm @Thickness 3.20 mm |
0.0025 - 0.0076 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Asia Pacific) 30% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Linear Mold Shrinkage, Transverse | 0.0025 cm/cm @Thickness 6.40 mm |
0.0025 in/in @Thickness 0.252 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 cm/cm @Thickness 6.40 mm |
0.0025 in/in @Thickness 0.252 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+PS LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0025 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL EM7304F PPE+PS 15% glass reinforced, high flow with enhanced polyurethane foam adhesion for instrument panel retainers. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 cm/cm | 0.0025 in/in | |
Toyobo TS101 PPS, Glass Fiber/Mineral Reinforced Key Feature: High dimensional stabilityHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 cm/cm | 0.0025 in/in | LATI |
LATI LASTIROL TR G/10-V1 10% Glass Fiber Reinforced Polystyrene (PS) (UL94 V-1)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 cm/cm | 0.0025 in/in | LATI |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0025 - 0.0050 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000A PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGN2000A compound is a 20% glass reinforced PC, high flow. UL rated V-0. Consumer Electronics applications. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 cm/cm | 0.0025 in/in | LATI |
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Lastil G/30 SAN, 30% Glass Fiber Reinforced Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. High dimensional stability. High stiffness.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Latilub 80-15T K/30 PPS, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0065 cm/cm | 0.0025 - 0.0065 in/in | |
LATI Latigea B01 I6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |