Industrial Laminates/Norplex NP320U Cotton Fabric

Category Polymer , Thermoset
Manufacturer Industrial Laminates/Norplex
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industrial Laminates/Norplex NP320U Cotton Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500"
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.40 g/cc

@Thickness 1.57 mm
1.30 - 1.40 g/cc

@Thickness 0.0620 in
ASTM D792
Moisture Absorption at Equilibrium 3.0 %

@Thickness 1.57 mm
3.0 %

@Thickness 0.0620 in
ASTM D229
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85 - 105

@Thickness 1.57 mm
85 - 105

@Thickness 0.0620 in
ASTM D785
Tensile Strength, Yield 62.1 MPa

@Thickness 1.57 mm
9000 psi

@Thickness 0.0620 in
CW; ASTM D638
89.6 MPa

@Thickness 1.57 mm
13000 psi

@Thickness 0.0620 in
LW; ASTM D638
Modulus of Elasticity 7.58 GPa

@Thickness 1.57 mm
1100 ksi

@Thickness 0.0620 in
CW; ASTM D229
10.3 GPa

@Thickness 1.57 mm
1500 ksi

@Thickness 0.0620 in
LW; ASTM D229
Flexural Strength 93.1 MPa

@Thickness 1.57 mm
13500 psi

@Thickness 0.0620 in
CW; ASTM D790
131 MPa

@Thickness 1.57 mm
19000 psi

@Thickness 0.0620 in
LW; ASTM D790
Compressive Strength 207 MPa

@Thickness 12.7 mm
30000 psi

@Thickness 0.500 in
ASTM D695
Shear Strength 82.7 MPa

@Thickness 15.7 mm
12000 psi

@Thickness 0.620 in
ASTM D732
Izod Impact, Unnotched 0.459 J/cm

@Thickness 12.7 mm
0.860 ft-lb/in

@Thickness 0.500 in
CW, Cond E-48/50; ASTM D256
0.587 J/cm

@Thickness 12.7 mm
1.10 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Flammability, UL94 HB

@Thickness 1.57 mm
HB

@Thickness 0.0620 in
Electrical Properties Metric English Comments
Dielectric Constant 6.6

@Thickness 1.57 mm
6.6

@Thickness 0.0620 in
Permittivity, Cond D-24/23; ASTM D150
Dielectric Strength 19.7 kV/mm

@Thickness 1.57 mm
500 kV/in

@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S.T.
24.6 kV/mm

@Thickness 1.57 mm
625 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Dielectric Breakdown 50000 V

@Thickness 1.57 mm
50000 V

@Thickness 0.0620 in
Cond A; ASTM D229 S/S
Dissipation Factor 0.054

@Thickness 1.57 mm
0.054

@Thickness 0.0620 in
Cond D-24/23; ASTM D150
Arc Resistance 15 sec

@Thickness 3.17 mm
15 sec

@Thickness 0.125 in
ASTM D495
Comparative Tracking Index 170 V

@Thickness 3.17 mm
170 V

@Thickness 0.125 in
ASTM D3638
Descriptive Properties Value Comments
Bond Strength 1700 lb
0.5", ASTM D229
Color Natural