Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group 3535 Epoxy Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | ISO 1183 |
Raschig Group 4552 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | ISO 1183 |
Raschig Group EPOXIDUR® 3580 EP Epoxy Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | ISO 1183 |
Raschig Group EPOXIDUR® 3582 EP Epoxy Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 4385 UP Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 4802 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 4806 UP Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 8602 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng.. |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group SURAPLAST 54 UPA Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | ASTM D792 |
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc @Thickness 1.57 mm |
1.90 - 2.00 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP130HF Glass Fabric Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | ASTM D297 |
Greene Tweed FPD Blueâ„¢ 707 Fluoroelastomer Specifically developed for flat panel display CVD and dry plasma etch equipment where seal reliability and minimal contamination are essential, FPD Blueâ„¢ 707 fluoroelastomer provides excellent .. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Lord Adhesives Thermosetâ„¢ ME-542 Underfill Encapsulant LORD Thermosetâ„¢ ME-542 encapsulant is an anhydridefree, thermally conductive, semiconductor grade epoxy underfill product developed for the encapsulation of densely populated area array flip ch.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | ASTM D-792 |
Glastic T-160 Fiberglass-Reinforced Polyester Laminate Grade T-160 is a new, high-strength, heat-resistant laminate. This highly creep-resistant material is excellent for applications where electrically insulating materials are subject to physical load.. |
|||
Specific Gravity | 1.90 - 1.96 g/cc | 1.90 - 1.96 g/cc | |
3M Dyneon™ FX 5912 Dynamar™ Polymer Processing Additive Dynamar FX 5912 is a free-flowing fluorothermoplastic processing aid that is designed for use at very low levels to improve the processing of thermoplastics. Typical use levels of 200 to 1000 ppm ha.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Aremco Pyro-Putty™ 653 High Temperature Ceramic-Metallic Putty, Stainless Filled Ceramic and Stainless-Filled, One-Part, Water Based Paste.For Vertical Surfaces and Applications to 1/2" Thick.Repairs Cast Iron, Steel and Stainless Parts to 2000°F. |
|||
Specific Gravity | 1.90 - 2.05 g/cc | 1.90 - 2.05 g/cc | |
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Bulk Molding Compounds BMC 5209 Mineral Filled, Glass Reinforced Polyester BMC 5209 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Specific Gravity | 1.90 - 1.93 g/cc | 1.90 - 1.93 g/cc | ASTM D792 |
Adamas Adalon® 410 PTFE+ PEEK Information provided by Adamas, HPM |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
BCC Products Kwik Kast BC 8650 Urethane Casting BC 8650 is an advanced fast cast polyurethane tooling system. BC 8650 features low viscosity, low exotherm and minimal shrinkage. Kwik Kast Blue cures hard, yet more durable resulting in less brittl.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Aremco AREMCOLOX™ 502-1600 (94%) Machinable Boron Nitride 94% Hot-pressed 94% boron nitride. High thermal conductivity. Easily machined. Non-reactive in molten salts, aluminum and other metals. Plates from 1/4" to 1" thick; rods from 1/4" to 3" diameter; b.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Specific Gravity | 1.90 - 2.00 g/cc | 1.90 - 2.00 g/cc | |
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | |
Parker Chomerics CHO-BOND 2167 Part B Silicone Information provided by Chomerics |
|||
Specific Gravity | 1.90 - 2.10 g/cc | 1.90 - 2.10 g/cc | ISO 1183 |
Raschig Group RALUPOL® 8605 UP Polyester Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire.. |
|||
Specific Gravity | 1.90 g/cc | 1.90 g/cc | ASTM D792 |
Saint-Gobain Fluran® F-5500-A Fluoroelastomer Tubing Fluran® Severe Environment Tubing has the physical and chemical characteristics that make it ideal for severe environments, such as dry cleaning fluid lines and solvent recovery systems, where othe.. |