Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass.. |
|||
Specific Gravity | 1.75 - 2.25 g/cc | 1.75 - 2.25 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL 1285 Conductive Elastomer Conductive Elastomer with Improved Corrosion Resistance. This conductive silicone elastomer features significantly improved corrosion resistance in salt spray environments over silver-plated copper-.. |
|||
Specific Gravity | 1.75 - 2.25 g/cc | 1.75 - 2.25 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6308 Conductive Elastomer Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Extruded onlyRoHS CompliantInformation.. |
|||
Specific Gravity | 1.75 - 2.25 g/cc | 1.75 - 2.25 g/cc | ASTM D792 |
Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by C.. |
|||
Specific Gravity | 1.75 - 1.76 g/cc | 1.75 - 1.76 g/cc | ASTM D792 |
Solvay Specialty Polymers Hylar® 5000 HG Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Hylar® 5000 HG is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong.. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
Premix Premi-Glas® 1265 VE 1265-VE (Compression Molded) Glass Reinforced Vinyl Ester TMC
(discontinued **)< Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti.. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-8451 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined.. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
Haysite HCR-125 Vinyl Ester Sheet, Corrosion Resistant HCR-125 is a corrosion resistant vinyl ester sheet created by impregnating fiber glass mat, synthetic surface veil, and inert additives with Derkane 470 resin and catalyst. A compression molded pro.. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer LNP* LUBRICOMP* KFL36 is a compound based on Acetal Copolymer resin containing 30% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp KFL36XXC Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL36 is an Acetal containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled Good WeatherabilityInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow 2200 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2200 is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2200 contai.. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow 2200 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2200 is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2200 contai.. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow 2200 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2200 is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2200 contai.. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Orange LL10257/4 Concentrate Based In LLDPE DescriptionPOLYBATCH® LL10257/4 is an orange color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® LL10257/4 is he.. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | |
Bulk Molding Compounds BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 685 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, oil .. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
Asahi Glass F-Clean® Film for Greenhouses F-CLEAN®, produced by Asahi Glass Company, Ltd., is a Ethylene-Tetrafluoroethylene copolymer (ETFE) film used as the preferred covering material for horticultural greenhouses. High ten.. |
|||
Specific Gravity | 1.75 - 1.85 g/cc | 1.75 - 1.85 g/cc | |
BCC Products METAL-KAST BC 8010 Urethane Casting New BC8010 is a quick setting urethane reproduction plastic system that simulates many of the desirable characteristics of aluminum metal. A highly machineable tooling material that is now easier to.. |
|||
Specific Gravity | 1.75 - 1.77 g/cc | 1.75 - 1.77 g/cc | ASTM D792 |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Specific Gravity | 1.75 - 2.05 g/cc | 1.75 - 2.05 g/cc | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 - 1.80 g/cc | 1.75 - 1.80 g/cc | ASTM D792 |
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **) Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Specific Gravity | 1.75 g/cc | 1.75 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Orange LL10257/4 Concentrate Based In LLDPE DescriptionPOLYBATCH® LL10257/4 is an orange color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® LL10257/4 is he.. |