Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Rigid Extrusion L8230 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Radici Radilon® A GV H0 30P Nylon 66-GF30 Automotive cooling liquid resistant PA66-GF30 grade designed to resist even in more severe operating condition. Indicated as "top of the class" material.Information provided by Radici group. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Radici Radilon® A RCV3015 RKC Nylon 66-GF30 Automotive cooling liquid resistant PA66-GF30 grade designed to be processed by GIT technology.Information provided by Radici group. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | |
Radici Radilon® A RV300R (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® 3412R PC (Asia Pacific) 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance Description: Injection Molding, PC+GF20%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Gromax BFG30-FH00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-8184 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1850/PL/15/BK PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Gromax BFG30-AH00B3 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.35 - 1.41 g/cc | 1.35 - 1.41 g/cc | ASTM D 792 |
Karina 753-35/1-Y-IS-SD Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Stir SpA Z 85 AT (PVC) Application: Beach platformsInformation provided by STIR SpA |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
Cheng Yu Plastic ML3420 PC, 20% Glass Fiber |
|||
Specific Gravity | 1.35 g/cc @Temperature 25.0 °C |
1.35 g/cc @Temperature 77.0 °F |
|
Dow Corning SILASTIC® V RTV SILICONE RUBBER BASE & CURING AGENT High strength silicone rubber featuring medium durometer, low mixed viscosity, suited for the reproduction of architectural, furniture components and prototypes. Silastic V is recommended for use wi.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
Ensinger TECATRON™ PPS Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
Colorite Polymers 8534 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | silicone property, side 2; Arlon SQA-TMS-024 |
Arlon 55141R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | |
Radici Radilon® A RV300 990 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | Part B; TM R050-16 |
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D-792 |
Axiall 2651 Rigid PVC, Molding Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D-792 |
Axiall 9129J Rigid PVC, Extrusion Georgia Gulf 9129J is designed for use in extruded price tag holders. The compound contains an ultraviolet light stabilizer which retards color change.Information provided by Georgia GulfGeorgia Gu.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Azoty Tarnow™ Tarnamid® T-27 GF25 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 25% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |