Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS Color Package may affect performance. Visual Fx PC+ABS in various metallic (Ares) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D 792 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible XV3902 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Specific Gravity | 1.18 - 1.24 g/cc | 1.18 - 1.24 g/cc | ASTM D792 |
S&E Specialty Polymers TufTech™ GM-3285 PVC Compound Application: A clear, FDA grade, PVC extrusion compound for general non-toxic or 75°C rated wire applications.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
Ineos Nova Zyntar® F7080 Developmental Flame Retardant Polystyrene
(discontinued **) Features: General purpose non-Deca based resin (does not combine with Decabromodiphenyloxide)Good indoor UV light color stability(grey colors)UL94 V-0 @ 1.5 mm for all colors Good aesthetics for inj.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D 792 |
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was suppli.. |
|||
Specific Gravity | 1.18 g/cc @Temperature 23.0 °C |
1.18 g/cc @Temperature 73.4 °F |
ASTM D792 |
Kingfa FRHIPS-960PC Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmNon-DPO, UV stabilityExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housingInforma.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
LG Chemical AF312 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
LG Chemical LUPOY EC5000AF PC/ABS, Flame Residence Description: Injection Molding, PC/ABS, Flame Residence, Anti-StaticApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 68928-70-1Information provided by LG Chemical |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | |
Momentive Performance Materials Addisilâ„¢ 1170 M Industrial Molding Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | |
Momentive Performance Materials RTV8111 Silicone Rubber Compounds for Potting, Encapsulating and Sealing RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS LNP* THERMOCOMP* CX05470 is a compound based on Polystyrene resin containing 20% Glass Fiber. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 3300-68 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
A. Schulman POLYBLAK™ 4663 Premium Conductive 40% Carbon Black Concentrate Based In Modified HDPE DescriptionPOLYBLAK® Black 4663 is a premium conductive carbon black concentrate containing 40% carbon black based in a modified HDPE carrier resin. This masterbatch is designed to provide a flexi.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Orange 1046E Concentrate Based In Polyethylene DescriptionPOLYBATCH® 1046E is an orange color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 1046E is .. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | |
Trelleborg Z500 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude Type: Estane® ETE 75DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
A. Schulman POLYBLAK™ 4663 Premium Conductive 40% Carbon Black Concentrate Based In Modified HDPE DescriptionPOLYBLAK® Black 4663 is a premium conductive carbon black concentrate containing 40% carbon black based in a modified HDPE carrier resin. This masterbatch is designed to provide a flexi.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | DIN 53479 |
Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | |
Colorite Polymers Vinylbond 95-950-65 PVC Compound Description: Vinylbond 95-950 series compounds are flexible PVC alloys which are formulated specifically for the window market industry. These compounds offer excellent bonding characteristics to ri.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
Bayshore Vinyl Compounds BVC 1204-70 Clear Vinyl Compound BVC 1204-70 Clear has been designed as a general purpose extrusion compound for use in spiral hose, window profiles and applications where high gloss is required. This material offers excellent ext.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 3202-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Caps, Closure, Connectors, Food Service Applications, Safety Equipment, Valves/Valve Parts Appearance-Cl.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
E-Polymers TEKALOY® G75NHT Brominated Flame Retardant High Impact PC/ABS Alloy PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan.. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® NH-1015 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
PolyOne Synprene® RT-3740 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection Molding.. |