Polymer Property : Specific Gravity = 1.24 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.18 - 1.24 g/cc
1.18 - 1.24 g/cc
ASTM D792
S&E Specialty Polymers TufTech™ GM-3285 PVC Compound
Application: A clear, FDA grade, PVC extrusion compound for general non-toxic or 75°C rated wire applications.Information provided by S&E Specialty Polymers
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D 792
Karina TR-450D42/347-C-IS PVC Compound
PVC Compound with addition of nitrile rubber recommended for injection of technical parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D 792
Karina 32/19-G Orange Color Concentrate for PVC
Color concentrate recommended for application in PVC compounds for general purposes injection. Recommended to use 2%.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.18 - 1.24 g/cc
1.18 - 1.24 g/cc
ASTM D 792
Karina 48/1-FC-LMP (SDB) Black Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
Specific Gravity 1.18 - 1.24 g/cc
1.18 - 1.24 g/cc
ASTM D 792
Karina 48/1-FC-LMP Black Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
Specific Gravity 1.18 - 1.24 g/cc
1.18 - 1.24 g/cc
ASTM D 792
Karina 55/200 Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D 792
Karina 550D48/1-A-IS-BZ Black PVC Compound
Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D 792
Karina 60/200 Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D 792
Karina 600D48/1-A-IS-BZ Black PVC Compound
Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.18 - 1.24 g/cc
1.18 - 1.24 g/cc
NBR NM-IEC 60811-1-3
Karina E 32/34-FC-LMP Orange Color Concentrate for PVC
Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. Important Con..
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D 792
Karina E 650D48/1 Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.19 - 1.24 g/cc
1.19 - 1.24 g/cc
ASTM D792
Spartech Royalite R71/920 PC/ABS Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
Specific Gravity 1.19 - 1.24 g/cc
1.19 - 1.24 g/cc
ASTM D792
Spartech Royalite R922 PC/ABS Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D792
Compuestos Dominicanos Polycom VG-410180 PVC Compound
Other flexible extrusion compounds are polycom VG which can be used to manufacture garden hoses of high gloss, clarity and outdoor resistance.Applications: Garden hose extrusion Appearance: Clear gr..
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D-792
Axiall 6710 Moldings & Extrusions Flexible PVC
Clear extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D-792
Axiall 8805 Moldings & Extrusions Flexible PVC
General purpose clear extrusion compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D-792
Axiall 18770 Moldings & Extrusions Flexible PVC
General purpose 105C, clear jacketing compound recommended for 1/32" wall and larger. Exhibits excellent migration properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat..
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D-792
Axiall 8542 Moldings & Extrusions Flexible PVC
General purpose, flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D-792
Axiall 8750 Moldings & Extrusions Flexible PVC
A clear, high quality extrusion and molding compound formulated to give good low temperature properties and good heat stability.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpora..
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D-792
Axiall 8751 Moldings & Extrusions Flexible PVC
Clear, UV stabilized extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D-792
Axiall 10757 Wire & Cable Flexible PVC
General purpose non-lead stabilized 75°C rated compound recommended for jacketing and general purpose extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporati..
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D-792
Axiall 19802 Wire & Cable Flexible PVC
Clear, 105°C rated extrusion compound recommended for 1/32" wall jacketing. Also well suited for injection molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpo..
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D-792
Axiall 8791 Moldings & Extrusions Flexible PVC
A quality extrusion and molding compound formulated for good low temperature properties, good UV resistance and excellent heat stability.Information provided by Georgia GulfGeorgia Gulf became Axial..
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D-792
Axiall 1701 Clear 7002 Flexible PVC
Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation ..
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D 792
Karina E 60/200 Cristal Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.20 - 1.24 g/cc
1.20 - 1.24 g/cc
ASTM D 792
Karina E 60/200-D Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.