Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBLAK™ 4663 Premium Conductive 40% Carbon Black Concentrate Based In Modified HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionPOLYBLAK® Black 4663 is a premium conductive carbon black concentrate containing 40% carbon black based in a modified HDPE carrier resin. This masterbatch is designed to provide a flexible range of electrical properties dependent on usage levels. POLYBLAK® Black 4663 offers exceptional durability and toughness for use in demanding industrial and automotive applications. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Carbon Black Loading 40 %
40 %
Electrical Properties Metric English Comments
Surface Resistance 1e+05
1e+05
50% let-down in HDPE
1.00e+7 ohm
1.00e+7 ohm
40% let-down in HDPE
Descriptive Properties Value Comments
Moisture (max) 1200
ppm, ASTM D789
Users viewing this material also viewed the following: