| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | Samsung, Cheil Industries |
| Trade Name | Infino® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Samsung Cheil Industries Infino® NH-1015 PC/ABS, Unreinforced FR.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
| Melt Flow | 24 g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C |
24 g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 61.8 MPa | 8960 psi | 50 mm/min; ASTM D638 |
| Flexural Strength | 86.3 MPa | 12500 psi | 2.8 mm/min; ASTM D790 |
| Flexural Modulus | 2.40 GPa | 348 ksi | 2.8 mm/min; ASTM D790 |
| Izod Impact, Notched | 5.88 J/cm <br>@Thickness 3.17 mm |
11.0 ft-lb/in <br>@Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 98.0 °C | 208 °F | B/50; ISO R306 |
| UL RTI, Electrical | 90.0 °C | 194 °F | |
| UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | |
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | |
| Flammability, UL94 | V-0 <br>@Thickness 1.50 mm |
V-0 <br>@Thickness 0.0591 in |
|
| 5VB <br>@Thickness 3.00 mm |
5VB <br>@Thickness 0.118 in |
||
| 5VA <br>@Thickness 2.00 mm |
5VA <br>@Thickness 0.0787 in |