Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable JJC32A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Dry Blend E7009 Polyvinyl Chloride, Rigid (PVC, Rigid) Recommended for whites and light pastel colors only. Not to be used for darker colors.Physical properties based on Geon E7009 white 1024 lot# UTCX 57572Information provided by PolyOne |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
Technetics Group Amicon™ PEEK 30% Glass Filled
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ AT-10CF/15T-2S Acetal-Copolymer, Carbon Fiber Reinforced, PTFE/Silicone Lubricated
(disco Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with .. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | DAM; ASTM D792 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-8167 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7720/BE PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
Fiberfil® M-2501 BK Nylon 66, 40% mineral Filled, post industrial Information provided by FIBERFIL Engineered Plastics |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | |
Sylvin Technologies 8980-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 2310 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 2310F PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM CRS5301 PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
Techmer ES Plaslube® AC-80/TF/20 BK1941 Acetal (POM) Copolymer |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow 2946ST Concentrate Based In Polyethylene DescriptionPOLYBATCH® 2946ST is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2946ST co.. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
Quantum PEI - Ultem® 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |