| Category | Polymer , Thermoplastic , Polyetherimide (PEI) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | ULTEM |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics ULTEM 2310F PEI.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.500 % | 0.500 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.90 % | 0.90 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 7.6 g/10 min @Load 6.60 kg, Temperature 337 °C |
7.6 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
| Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 360 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 158 MPa | 22900 psi | Type I, 5 mm/min; ASTM D638 |
| 165 MPa | 23900 psi | 5 mm/min; ISO 527 | |
| Tensile Strength, Yield | 165 MPa | 23900 psi | 5 mm/min; ISO 527 |
| 168 MPa | 24400 psi | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Break | 2.0 % | 2.0 % | 5 mm/min; ISO 527 |
| 3.0 % | 3.0 % | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Yield | 2.0 % | 2.0 % | 5 mm/min; ISO 527 |
| 3.0 % | 3.0 % | Type I, 5 mm/min; ASTM D638 | |
| Tensile Modulus | 9.23 GPa | 1340 ksi | 5 mm/min; ASTM D638 |
| 9.50 GPa | 1380 ksi | 1 mm/min; ISO 527 | |
| Flexural Strength | 220 MPa | 31900 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
| Flexural Yield Strength | 220 MPa | 31900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 225 MPa | 32600 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 8.50 GPa | 1230 ksi | 2 mm/min; ISO 178 |
| 9.25 GPa | 1340 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
| 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| 4.37 J/cm @Thickness 3.20 mm |
8.19 ft-lb/in @Thickness 0.126 in |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1A |
| 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Dart Drop, Total Energy | 10.0 J @Temperature 23.0 °C |
7.38 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 16.0 µm/m-°C @Temperature -20.0 - 150 °C |
8.89 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
| 16.0 µm/m-°C @Temperature 23.0 - 150 °C |
8.89 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 41.0 µm/m-°C @Temperature -20.0 - 150 °C |
22.8 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
| 41.0 µm/m-°C @Temperature 23.0 - 150 °C |
22.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 208 °C @Thickness 3.20 mm |
406 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| 210 °C @Thickness 6.40 mm |
410 °F @Thickness 0.252 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
| 220 °C | 428 °F | Rate B/120; ISO 306 | |
| 228 °C | 442 °F | Rate B/50; ASTM D1525 | |
| Glass Transition Temp, Tg | 217 °C | 423 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | Passes | IEC 60695-10-2 |