Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
PolyOne Nymax™ GF 600 A 44 Black 13 Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
PolyOne Nymax™ GMF 600 A 40 Natural Polyamide 6 (Nylon 6) The Nymax® 600 Series of mineral-reinforced nylon 6 compounds have been specifically developed to provide an excellent balance of physical property performance and durability, with improved surface.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC AMC™ 8595 is a vinyl ester engineered structural composite molding compound with continuous, unidirectional carbon fibers. It is designed for compression molding of components requiring high struc.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Polymer Resources PC-G40 Polycarbonate, 40% Glass Reinforced Polycarbonate, 40% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Polymer Resources TPSF-G30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet) |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Fiberfil® PP-60/TC/20/VO/ND Polypropylene Homopolymer, 20% Talc Filled, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Specific Gravity | 1.50 - 1.60 g/cc | 1.50 - 1.60 g/cc | ASTM D1475 |
Lotus Nano Paint NAP 301 Airport Nano-paint Description: This grade of traffic marking nano-paints is a fast dry and has better reflection of light. Because of these specifications these paint are suitable for Airports and inter-city roads. T.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Loxim 340 01HB Nylon 6 Information provided by Loxim Industries |
|||
Specific Gravity | 1.50 - 1.56 g/cc | 1.50 - 1.56 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 42/6-FC-LMP Red Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | |
Sylvin Technologies 9980-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D 792 |
SABIC Innovative Plastics Valox® VC130 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Samyang Tribit® 1500G15 Polybutylene Terephthalate, 15% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Samyang Tribit® 1500G15K PBT, Reinforced Impact Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G15K is a reinforced, impact grade.Appl.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | Mixed |
Tra-Con Tra-Cast 3101 Encapsulating Adhesive System TRA-CAST 3101 is an easy-to-use, room temperature cure, rigid, low viscosity, 100% solids (no solvents) epoxy resin and hardener system with excellent mechanical and electrical properties. It is rec.. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Cheng Yu Plastic NG1400S Nylon 66, 40% Glass Fiber Reinforced |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D792 |
Diamond Polymers DIAMALOY 508 30% Glass Filled PC/Polyester Alloy, UV Stabilized Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ISO 1183 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Specific Gravity | 1.50 g/cc @Temperature 23.0 °C |
1.50 g/cc @Temperature 73.4 °F |
ASTM D792 |
Asia International Enterprise (Hong Kong) 60G8 Nylon 66, 40% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | ASTM D-792 |
Axiall 7407 Rigid PVC, Extrusion Georgia Gulf 7407 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.50 g/cc | 1.50 g/cc | Dry; ASTM D792 |
Asahi Kasei Leona® 13G43 43% Glass Filled Nylon 66 43% Glass Fiber Reinforced. Enhanced strength and stiffnessApplications:Mechanical and electrical parts such as micromotors, automotive parts such as radiator tanks and shift leversInformation provi.. |
|||
Specific Gravity | 1.50 - 1.80 g/cc | 1.50 - 1.80 g/cc | IEC 1212-2 7.2 |
Hippe PF GC 21 Woven Glass Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Very high mechanical strength at moderate temperatures.Information provided by Hippe. |