Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
PolyOne Geon™ Vinyl Rigid Molding M5005 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
PolyOne Geon™ Vinyl Wire & Cable W1820L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
PolyOne LubriOne™ AT-000/05T Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Quadrant EPP Techtron® HPV PPS (ASTM Product Data Sheet)
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Ravago Manufacturing Americas Hylex® P1310G30 HB Polycarbonate, 30% Fiberglass Reinforced, UV Stabilized
Information provided by Ravago.
Specific Gravity 1.43 g/cc
1.43 g/cc
PBI Performance Products Celazole® TL-60 Self Lubricating Melt Processable Polybenzimidazole
Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. ..
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
PolyOne Edgetek® PS-30CF/000 HF UV BLACK Polybutylene Terephthalate (PBT)
Information provided by PolyOne
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
SABIC Innovative Plastics Lexan® FL930 PC (Asia Pacific)
Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm).
Specific Gravity 1.43 - 1.49 g/cc
1.43 - 1.49 g/cc
NBR NM-IEC 60811-1-3
Karina E900D10/1-E-IS-BZ White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.43 g/cc
1.43 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1850/CF/15/TF/10/EM PBT, with carbon fiber, PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita..
Specific Gravity 1.43 g/cc
1.43 g/cc
ISO 1183
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber
PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS.
Specific Gravity 1.43 g/cc
1.43 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1105-7781 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
LG Chemical LUPOY GN2301F PC+GF30%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF30%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
Specific Gravity 1.43 g/cc
1.43 g/cc
Silberline A-6205
A-6205 is a standard grade; class B, medium sized, leafing aluminum pigment carried in C-66 exempt mineral spirits.Applications: Trade & Maintenance
Specific Gravity 1.43 g/cc
1.43 g/cc
Silberline A-6211
A-6211 is a standard grade; class B, medium sized, leafing aluminum pigment carried in C-66 exempt mineral spirits.Applications: Trade & Maintenance
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK3020 PC
LNP* Thermocomp* Lexan_LGK3020 compound is a glass reinforced. Flame retardant.
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Samyang Trirex® 3500G30 Polycarbonate, 30% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Teknor Apex APEX® 327 Polyvinyl Chloride, Flexible
Notes: 60°C Insulation; RoHS Compliant Uses: Flexible Cord Insulation; Flexible Cord JacketingForms: Pellets Wire Types: SJT; SPT-1; SPT-2; SPT-3; SRDT; ST; SVT Agency Ratings: UL 1581; UL 62 Pro..
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
A. Schulman POLYBATCH™ Canyon 10277U/4 Concentrate Based In LLDPE
DescriptionPOLYBATCH® 10277U/4 is a canyon color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provided color and UV stabil..
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
A. Schulman POLYBATCH™ Canyon 10290U/4 Concentrate Based In LLDPE
DescriptionPOLYBATCH® 10290U/4 is a canyon color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabilit..
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
A. Schulman POLYBATCH™ Treated Pine 60181U/4 Concentrate Based In LLDPE
DescriptionPOLYBATCH® 60181U/4 is a treated pine color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV s..
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
A. Schulman POLYBATCH™ Treated Pine 60181U/4 Concentrate Based In LLDPE
DescriptionPOLYBATCH® 60181U/4 is a treated pine color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV s..
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Daelim H&L Plavis-G15 DF 15% Graphite Filled Aromatic Polyimide Bearing
Direct Formed. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 ca..
Specific Gravity 1.43 g/cc
1.43 g/cc
Absolute Drying; ASTM-D792
Toyobo GLAMIDE® T-779 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..