Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1105-7781 PEEK, with carbon fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Lehmann & Voss LUVOCOM® 1105-7781 PEEK, with carbon fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically conductive, suitable for continuous discharging of statically generated electricity.Bearings, sleeves, control disks, gear wheels, pump impellers, gear parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm
0.0010 - 0.0040 in/in
Melt Flow <= 14.3 g/10 min

@Load 10.0 kg,
Temperature 380 °C
<= 14.3 g/10 min

@Load 22.0 lb,
Temperature 716 °F
Mechanical Properties Metric English Comments
Tensile Stress 240 MPa
34800 psi
Elongation at Yield 1.8 %
1.8 %
2.3 %
2.3 %
flexural
Modulus of Elasticity 26.0 GPa
3770 ksi
Flexural Strength 350 MPa
50800 psi
Flexural Modulus 22.0 GPa
3190 ksi
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
flatwise; ISO 179 1fU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179 1eA
Thermal Properties Metric English Comments
CTE, linear 9.00 µm/m-°C
5.00 µin/in-°F
DIN 53752
Thermal Conductivity 0.600 W/m-K
4.16 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 250 °C
482 °F
280 °C
536 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
Flammability, UL94 V-0
V-0
not recognized by UL
Electrical Properties Metric English Comments
Surface Resistance <= 10000 ohm
<= 10000 ohm
Insulation Resistance <= 100000 ohm
<= 100000 ohm
Processing Properties Metric English Comments
Processing Temperature 390 °C
734 °F
mass temp
Nozzle Temperature 360 - 380 °C
680 - 716 °F
Zone 1 360 - 370 °C
680 - 698 °F
Zone 2 380 - 390 °C
716 - 734 °F
Zone 3 390 - 400 °C
734 - 752 °F
Mold Temperature 170 - 200 °C
338 - 392 °F
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
150 °C

@Time 10800 - 21600 sec
302 °F

@Time 3.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color (black)
Users viewing this material also viewed the following: