| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Unreinforced, Molded |
| Manufacturer | PolyOne Corporation |
| Trade Name | Edgetek® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Edgetek® PS-30CF/000 HF UV BLACK Polybutylene Terephthalate (PBT).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.020 - 0.060 cm/cm @Thickness 3.18 mm |
0.020 - 0.060 in/in @Thickness 0.125 in |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.011 - 0.013 cm/cm @Thickness 3.18 mm |
0.011 - 0.013 in/in @Thickness 0.125 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 165 MPa | 23900 psi | 5.1 mm/min; ASTM D638 |
| Elongation at Break | 1.0 - 2.0 % | 1.0 - 2.0 % | ASTM D638 |
| Tensile Modulus | 21.9 GPa | 3180 ksi | 5.1 mm/min; ASTM D638 |
| Flexural Strength | 255 MPa | 37000 psi | 1.3 mm/min; ASTM D790 |
| Flexural Modulus | 17.9 GPa | 2600 ksi | 1.3 mm/min; ASTM D790 |
| Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 222 °C | 432 °F | Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 211 °C | 412 °F | Unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 100 - 10000 ohm-cm | 100 - 10000 ohm-cm | ASTM D257 |
| Surface Resistance | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Electrically Conductive | |
| Good Chemical Resistance | ||
| Good Flow | ||
| High Heat Resistance | ||
| High Stiffness | ||
| Semi Crystalline | ||
| Filler / Reinforcement | Carbon Fiber Reinforcement, 30% Filler by Weight | |
| Forms | Pellets | |
| Generic Material | PBT | |
| Generic Name | Polybutylene Terephthalate (PBT) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Appliance Components | |
| Appliances | ||
| Automotive Applications | ||
| Consumer Applications | ||
| Housings | ||
| Industrial Applications | ||
| Structural Parts |