Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
Polymax® Maxelast® P3890 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
PolyOne Elastamax™ XL-2155 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | 23/23°C; ASTM D792 |
RheTech Products M15P101-01 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
LG Chemical HI100H ABS, High Impact, High Toughness Feature: Injection Molding, High Impact, High ToughnessApplication: Helmet, Pipe & Fittings)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | Resin |
Taiwan PU Corporation TPUCO Polyurethane Sealing Resin PU sealing resin is a waterproof, insulated protective film made of quality PU resin. It is used in the prevention of humidity, germs, collision, corrosion, parts loosening, and rusting, and as ins.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | foam molded; ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC3008A PPE+PS LNP* Stat-kon* Noryl_FMC3008A compound is a 30% carbon fiber/glass/mineral filled, static dissipative, foamable resin. UL94 V1 rated. Property values at 20% weight reduction, 0.250"" wall. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2336UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
Teknor Apex Telcar® OBC 4560A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Specific Gravity | 1.02 - 1.06 g/cc | 1.02 - 1.06 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ ASP-2000 Permanent Antistatic Product DescriptionPOLYBATCH® ASP-2000 is a permanent antistatic product. This material is designed to provide immediate antistatic performance and last throughout the lifetime of the polyolefin. POLYBAT.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 397 Ionomer Information provided by A. Schulman. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ISO 1183 |
Ter Hell Plastic K-Resin KRE 9902 Butadiene-Styrene Copolymer Description: Butadiene-Styrene Copolymer Compound, good transparency with impact strength and stiffness well-balanced.Application: For all kinds of injection molded parts.Information provided by T.. |
|||
Specific Gravity | 1.02 g/cc @Temperature 25.0 °C |
1.02 g/cc @Temperature 77.0 °F |
|
Dow Corning MOLYKOTE® PG-54 PLASTISLIP GREASE Silicone grease with solid lubricantsInformation provided by Dow Corning |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | Part B |
Epoxy Technology EPO-TEK® 353ND Black High Temperature Epoxy Product Description: EPO TEK® 353ND Black is a a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applicationsAdvantages & Application Notes: EPO T.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | Part B |
Epoxy Technology EPO-TEK® 431 Copper Filled Epoxy A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding and EMI RF shielding... |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | Part B |
Epoxy Technology EPO-TEK® OE100-T High Temperature Epoxy Material Description: A two component, high Tg, high temperature grade epoxy designed for semiconductor, underfill, hard-disk drive and hybrid micro-electronics packaging applications. The epoxy ca.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | |
Dow SPECFLEX™ NC 632 Polyol SPECFLEX™ NC 632 polyol is a specialty capped polyol. Its high molecular weight and primary hydroxyl content make it well suited for high resilience, flexible molded foams. CAS# 009082-00-2 0.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
Buckeye Polymers BP FLEX D5718 TU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | "A" component |
ACC QLE 1020 QSI Quantum Silicones 45 Durometer Clear, Addition Cure Elastomer for Coating QLE 1020 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | "A" component |
ACC QLE 1039 QSI Quantum Silicones 40 Durometer Addition Cure Elastomer for Coating QLE 1039 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |
|||
Specific Gravity | 1.02 g/cc | 1.02 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Green 30424 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 30424 is a green color concentrate based in polyethylene. This concentrate was designed to provide color in blow molding and injection molding applications. POLYBATCH® 3042.. |
|||
Specific Gravity | 1.02 - 1.08 g/cc | 1.02 - 1.08 g/cc | ASTM D792 |
Spartech Royalite R12 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |