A. Schulman POLYBATCH™ ASP-2000 Permanent Antistatic Product

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ ASP-2000 Permanent Antistatic Product.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® ASP-2000 is a permanent antistatic product. This material is designed to provide immediate antistatic performance and last throughout the lifetime of the polyolefin. POLYBATCH® ASP-2000 will not bloom to the surface and will therefore not interfere with printing. POLYBATCH® ASP-2000 performance is maximized when processed at temperatures between 190 to 230°C (375 to 446°F). ApplicationPOLYBATCH® ASP-2000 is typically recommended for us in blown film, injection molding, and blow molding applications at 10 to 15% addition levels depending upon application requirements. This product is not recommended for use in cast film applications.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792