Material Notes:
QLE 1020 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: 100% solids Long open time Excellent adhesion Clear, but can be tinted Good abrasion resistancePart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
"B" component
1.02 g/cc
1.02 g/cc
"A" component
Viscosity 6000 cP
6000 cP
"B" component
50000 cP
50000 cP
"A" component
Storage Temperature <= 38.0 °C
<= 100 °F
12 months
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
cured 60 mins @ 150°C
Tensile Strength, Yield 3.40 MPa
493 psi
cured 60 mins @ 150°C
Elongation at Break 260 %
260 %
cured 60 mins @ 150°C
Tear Strength 8.77 kN/m
50.0 pli
cured 60 mins @ 150°C
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Gel Time >= 4320 min
>= 4320 min
Catalyzed
Descriptive Properties Value Comments
Color Clear
"A" component
Clear
"B" component