Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.02 - 1.08 g/cc | 1.02 - 1.08 g/cc | ASTM D792 |
S&E Specialty Polymers GTPR-1358A Thermoplastic Rubber material designed for winter boot applications requiring excellent abrasion and stitch tear. Available in a wide range of colors.Information provided by S&E Specialty Polymer.. |
|||
Specific Gravity | 1.02 - 1.08 g/cc | 1.02 - 1.08 g/cc | Uncured |
Resin Technology Group UV-403 High Clarity, Structural Polycarbonate and PVC Bonder UV 403 is a very fast UV curing adhesive developed for bonding a variety of plastics. Bond strengths on polycarbonate and rigid PVC usually exceed the strength of those substrates. Bond lines are cl.. |
|||
Specific Gravity | 1.06 - 1.08 g/cc | 1.06 - 1.08 g/cc | |
Michelman® CleanGrip® 2100 Silica based, sprayable nonskid coating Description: Water based frictionizing agentUsage: CleanGrip® 2100 is a silica based, sprayable nonskid coating designed to reduce the slipperiness of shipping containers by providing excellent s.. |
|||
Specific Gravity | 1.06 - 1.08 g/cc | 1.06 - 1.08 g/cc | |
Michelman® Hydrosize® HP3-02 Nonionic phenoxy dispersion Description: Nonionic phenoxy dispersionUsage: Hydrosize® HP3-02 is designed to be used as a fiber sizing coating with a high Tg and excellent adhesion.When manufactured in USA product meets food.. |
|||
Specific Gravity | 1.06 - 1.08 g/cc | 1.06 - 1.08 g/cc | |
Michelman® Licomer® A 53 Acrylic polymer dispersion Description: Acrylic polymer dispersionUsage: Licomer® A 53 is an aqueous polymer dispersion for the manufacture of dry-bright emulsions intended especially for the care of floors. This product p.. |
|||
Specific Gravity | 1.06 - 1.08 g/cc | 1.06 - 1.08 g/cc | |
Michelman® Licomer® T 51 Acrylic copolymer dispersion Description: Acrylic copolymer dispersion, metal containingUsage: Licomer® T 51 is a dispersion suitable for dry-bright emulsions and cleaning products due to high transparency and hardness. This.. |
|||
Specific Gravity | 1.06 - 1.08 g/cc | 1.06 - 1.08 g/cc | |
Michelman® Michem® Emulsion 48625M1 Polymer solution Description: Polymer solutionUsage: Michem® Emulsion 48625M1 is a sizing polymer for fiberglass and other fibers serving as reinforcement for various resins.We serve many markets through MichemÂ.. |
|||
Specific Gravity | 1.02 - 1.08 g/cc | 1.02 - 1.08 g/cc | ASTM D 792 |
Karina E 4800/3-IE MBPEBD Black Color Concentrate Black pigment concentrate recommended for polyolefins application and polyolefins compounds.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.06 - 1.08 g/cc | 1.06 - 1.08 g/cc | |
Michelman® Licomer® M 55 Styrene-Acrylate copolymer dispersion Description: Styrene-Acrylate copolymer dispersion, metal containingUsage: Licomer® M 55 is an aqueous polymer dispersion for the manufacture of dry-bright emulsions intended especially for the c.. |
|||
Specific Gravity | 1.06 - 1.08 g/cc | 1.06 - 1.08 g/cc | |
Michelman® Licomer® M 63 Styrene-Acrylate copolymer dispersion Description: Styrene-Acrylate copolymer dispersion, metal containingUsage: Licomer® M 63 is an aqueous polymer dispersion for the manufacture of dry-bright emulsions intended especially for the c.. |
|||
Specific Gravity | 1.02 - 1.08 g/cc | 1.02 - 1.08 g/cc | ASTM D792 |
Spartech Royalite R20 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.02 - 1.08 g/cc | 1.02 - 1.08 g/cc | ASTM D792 |
Spartech Royalite R21 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.02 - 1.08 g/cc | 1.02 - 1.08 g/cc | ASTM D792 |
Spartech Royalite R24 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.02 - 1.08 g/cc | 1.02 - 1.08 g/cc | ASTM D792 |
Spartech Royalite R26 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.03 - 1.08 g/cc | 1.03 - 1.08 g/cc | ASTM D792 |
Spartech Royalite R84 Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.02 - 1.08 g/cc | 1.02 - 1.08 g/cc | ASTM D792 |
Buckeye Polymers BP RPPC 2010 CW Polypropylene, Calcium Filled Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges fro.. |
|||
Specific Gravity | 1.01 - 1.08 g/cc | 1.01 - 1.08 g/cc | ASTM D792 |
Buckeye Polymers BP RPP 2012 TR BLK Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
Specific Gravity | 1.01 - 1.08 g/cc | 1.01 - 1.08 g/cc | ASTM D792 |
Buckeye Polymers BP RPPC 1720 TURXF Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
Specific Gravity | 1.02 - 1.08 g/cc | 1.02 - 1.08 g/cc | ASTM D792 |
Spartech Royalite R12 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |