Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N1300HL BK/UV2 Post Consumer Recycle Nylon 66 Heat Stabilized, Lubricated, UV Stabilized, Black and made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N1300STHL Post Consumer Recycle Nylon 66 Superior Toughness, Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N2300HL BK Post Consumer Recycle Nylon 6 Heat Stabilized, Lubricated, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N2300HL BK/UV2 Post Consumer Recycle Nylon 6 Heat Stabilized, Lubricated, UV Stabilized, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N2300THL BK/HF Post Consumer Recycle Nylon 6 Impact Modified, High Flow, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.019 cm/cm @Thickness 3.17 mm |
0.014 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000HL Nylon 6/6 Available in North America Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and Lubricated RoHS Compliant Auto Specifications: FORD WSK-M4D648-A Color: Black Form: Pellets Processi.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.019 cm/cm | 0.013 - 0.019 in/in | ASTM D955 |
PolyOne Dynaflex™ G7950-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7950-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.019 cm/cm | 0.013 - 0.019 in/in | ASTM D955 |
PolyOne Dynaflex™ G7950-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7950-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B70CA Polyvinyl Chloride, Flexible (PVC, Flexible) Improved adhesion.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B70CB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A80U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N1300THL BK Post Consumer Recycle Nylon 66 Impact Modified, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.20 mm |
0.015 - 0.019 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.20 mm |
0.015 - 0.019 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.0155 - 0.019 cm/cm | 0.0155 - 0.019 in/in | |
LATI Latilub 73/13-10T Y/15 POM, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE. Aramid fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust.. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.019 cm/cm | 0.017 - 0.019 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66 (Europe-Africa-Middle East) LNP* Verton* RL002 is a compound based on Nylon 66 resin containing PTFE. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.019 cm/cm @Thickness 3.20 mm |
0.012 - 0.019 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East) Valox 7062 is Mineral filled PBT injection molding grade. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.019 cm/cm @Thickness 3.20 mm |
0.012 - 0.019 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.019 cm/cm | 0.0060 - 0.019 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.019 cm/cm @Thickness 3.20 mm |
0.012 - 0.019 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Linear Mold Shrinkage, Flow | 0.0060 - 0.019 cm/cm | 0.0060 - 0.019 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22LHI6 XE-NBK1 Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.019 cm/cm | 0.017 - 0.019 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1733-GY1 Lubricated, Nucleated, Unfilled Nylon 6 Description: Lubricated, Nucleated, Unfilled Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66 Description: Medium Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.019 cm/cm | 0.014 - 0.019 in/in | ASTM D955 |
Clariant Renol 6608 HSL Nylon 66, High Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N2300STHL BK Post Consumer Recycle Nylon 6 Superior Toughness, Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.019 cm/cm | 0.017 - 0.019 in/in | ASTM D955 |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), .. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | DIS 294-4 |
Wellman Wellamid® 42LH-WBK Nylon 6, Engineering Grade All information provided by Wellman Engineered Resins. |