Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.022 - 0.026 cm/cm | 0.022 - 0.026 in/in | ASTM D955 |
PolyOne Dynaflex™ G7736-1 Thermoplastic Elastomer (TPE) Dynaflex™ G7736-1 is a general purpose compound designed to provide easy processing and a good surface finish. - Good Aesthetics - Good Ozone/UV Stability - High Flow for Thin-Wall Parts - Overmold.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | 60x60x2; 260°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Pocan® B 5220 XF 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, improved flowability, improved impact strength, low tendency to warpInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 3.17 mm |
0.022 in/in @Thickness 0.125 in |
1/8" Section |
Lucent Polymers POM-270 Acetal Copolymer, Easy Flow, Injection Grade Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.032 cm/cm | 0.022 - 0.032 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP KL002 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KL002 is a compound based on Acetal Copolymer resin containing PTFE. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 3.17 mm |
0.022 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® HDPE TM10 10% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.026 cm/cm | 0.022 - 0.026 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Noryl GTX LMX171 PPO/PBT (Europe-Africa-Middle East) Noryl LMX171 is a PPO/PBT blend including conductive agent with a balanced heat/impact property profile. Noryl LMX differentiate from Noryl GTX by a lower moisture uptake (0.15%).This data was suppl.. |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.032 cm/cm | 0.022 - 0.032 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer Elastocon® 2810 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2810 is FDA compliant and well suit.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 2.00 mm |
0.022 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® S600LF NC010 PBT Crastin® S600LF NC010 is an unreinforced, Teflon® PTFE powder lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.022 - 0.024 cm/cm @Thickness 4.00 mm |
0.022 - 0.024 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Clariant CA9000NAT` Acetal Copolymer Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Diameter 2.00 mm |
0.022 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, Conditioned Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Diameter 2.00 mm |
0.022 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® RH190TB Acetal Impact modified reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity, black.Data provided by the manufacturer |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm @Thickness 3.20 mm |
0.022 in/in @Thickness 0.126 in |
|
Unitika ET2025 PA6, Dry High-impact nylonInformation provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it .. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® RH190 Acetal General purpose, reprocessed homopolymer, excellent toughness, strength, stiffness and lubricity. Available in Natural and Black. Natural: Designated RH190N-3; Black: Designated RH190B.Data provid.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® R190H Acetal General purpose, reprocessed copolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for good weatherability. Available in Natural and Black. Natural: Designated R190H-N3.. |
|||
Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
Ashley Polymers Ashlene® R190H2 Acetal General purpose economy grade copolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for maximum weatherability. Available in Natural and Black. Natural: Designated R190.. |