Polymer Property : Linear Mold Shrinkage, Flow = 0.011 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.011 - 0.014 cm/cm
0.011 - 0.014 in/in
ASTM D955
PolyOne Nymax™ 1280 A HS Black 11 A Polyamide 66 (Nylon 66)
The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi..
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Thickness 3.17 mm
0.011 in/in

@Thickness 0.125 in
ASTM D955
Network Polymers Softflex® 0615
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
ASTM D955
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation..
Linear Mold Shrinkage, Flow 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical KEYFLEX BT 1055D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical KEYFLEX BT 1163D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Thickness 3.20 mm
0.011 - 0.013 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical LUPOL HI5302A PP+MF15%, High Impact
Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.011 - 0.014 cm/cm
0.011 - 0.014 in/in
LATI Latene® EP 22UVH2 MX/25 PP Copolymer, Mineral Reinforced
Polypropylene copolymer (PPc) based compound. UV stabilized. Improved thermal stabilization. Special mineral filler. Very good surface appearance. Good elongation.Availability: Africa & Middle East;..
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP HAL23 PA11 (Europe-Africa-Middle East)
LNP* LUBRICOMP* HAL23 is a compound based on PA 11 resin containing Aramid Fiber, PTFE. Added features include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
Solvay TECHNYL® B 50 H1 PA66/6, DRY
Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av..
Linear Mold Shrinkage, Flow 0.011 - 0.020 cm/cm
0.011 - 0.020 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East)
VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Thickness 3.17 mm
0.011 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill FR® PA6/6 FR NAT
Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Thickness 3.17 mm
0.011 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PA6 E2
Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.011 - 0.015 cm/cm

@Time 86400 sec
0.011 - 0.015 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermotuf R1000EI2 PA 66 (Asia Pacific)
High Impact Nylon 66 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Thickness 3.20 mm
0.011 - 0.013 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA
Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance.
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm

@Thickness 3.20 mm
0.011 - 0.013 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics NORYL GTX GTX6011 PPE+PA6 (Asia Pacific)
PA6 based unfilled GTX. High impact.
Linear Mold Shrinkage, Flow 0.011 - 0.014 cm/cm
0.011 - 0.014 in/in
ISO DIS 294-4
Wellman Wellamid® GF10-42LI4-N-Gray 10% Glass Reinforced, Toughened Nylon 6
Description: Glass Reinforced, Toughened Nylon 6Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
ISO DIS 294-4
Wellman Wellamid® NY1599-BK11 Unfilled Nylon 66
Description: Unfilled Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Thickness 3.00 mm
0.011 in/in

@Thickness 0.118 in
MD
Toyobo VYLOPET® EMC605P PBT/PET Alloy, Anti-microbial
Applications: Gas equipment partsFeatures: Good anti-microbialGood appearanceFlame resistantInformation provided by Toyobo.
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® BFZ 3 PA6
Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties: Extreme toughnessEasy processingLow density Gril..
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
Eurotec
Eurotec® Tecomid® NB30 BK EF PA6, unfilled, black, suitable for electrostatic powder coating
Information provided by Eurotec®
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
Eurotec
Eurotec® Tecomid® NB40 NL FY70 PA6, flame retardant - halogen free (RoHS compliant), natural
Information provided by Eurotec®
Linear Mold Shrinkage, Flow 0.011 - 0.021 cm/cm
0.011 - 0.021 in/in
ASTM D955
Elastocon TPE Technologies Elastocon® 8150B Thermoplastic Elastomer
Elastocon® 8150B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8150B is well suited for consumer goods a..
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
DAM; ISO 294-4
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Linear Mold Shrinkage, Flow 0.011 cm/cm

@Thickness 3.20 mm
0.011 in/in

@Thickness 0.126 in
DAM
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
BASF Procom® D 1175 Polypropylene
Data was collected by ISO methods and provided by BASF.
Linear Mold Shrinkage, Flow 0.011 - 0.015 cm/cm
0.011 - 0.015 in/in
ISO DIS 294-4
Wellman Wellamid® MRB40K004-WT1 40% Mineral Reinforced Nylon 66
Description: Mineral Reinforced Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.011 - 0.014 cm/cm
0.011 - 0.014 in/in
ISO 294-4
Polyplastic Armlen® PP MF 40-2HS Polypropylene, 40% Mineral Filled
Impact modified, injection moldingInformation provided by PolyPlastic Group.
Linear Mold Shrinkage, Flow 0.011 - 0.014 cm/cm
0.011 - 0.014 in/in
LATI Latimass 52/11-04 D008 PP Homopolymer
Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati..
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® BZ 1 PA6
Information provided by EMS Grivory