Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Rigid Molding M5015 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Rigid Molding M5200 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
PolyOne Maxxam™ DP-8463-7001 Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0035 cm/cm | 0.0020 - 0.0035 in/in | |
Ovation Polymers Opnyl OP66GF50 Nylon 66 Nylon 66-Glass reinforced(50%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D955 |
Ravago Manufacturing Americas Hylex® P1310G15 HB Polycarbonate, 15% Fiberglass Reinforced, UV Stabilized Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | ASTM D955 |
PolyOne Nymax™ GF 600 A 33 Black 13 Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Cycoloy® C4220 PC+ABS (Europe-Africa-Middle East) CYCOLOY C4220 is a 20% glass reinforced, non FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance that combines a good processabity with a lo.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP DCL32 PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DCL32 is a compound based on Polycarbonate resin contqaining Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0060 in/in @Thickness 0.126 in |
|
Eastman Tenite 131E-28 Cellulose Acetate
(discontinued **) 28% plasticized and contains 50% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm @Temperature 80.0 °C |
0.0020 in/in @Temperature 176 °F |
60x60x2 mm; ISO 294-4 |
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm @Thickness 3.18 mm |
0.0020 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm @Thickness 3.17 mm |
0.0020 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 GF33 BK024 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | GB/T 15585-1995 |
Sichuan Deyang Haton® hGR50 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0060 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Europe-Africa-Middle East) NORYL GFN2 is a standard 20 % glass fibre reinforced material with a HDT/A of 130C according ISO 75. NORYL GFN2 can be used for all applications where a higher modulus is required. NORYL GFN2 is ava.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm @Thickness 3.17 mm |
0.0020 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PSU GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | ASTM D955 |
Chase Plastics CP Pryme® NN133LUV (Dry) Nylon 66, 33% Glass Fiber Reinforced, Lubricated, UV Stabilized Features: Good chemical resistanceGrease resistantLubricatedOil resistantHigh rigiditySolvent resistantHigh tensile strengthGood UV resistanceForm: PelletsApplications: Automotive under the hoodOutd.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm @Thickness 3.20 mm |
0.0020 in/in @Thickness 0.126 in |
|
Unitika B2040G50 PA66, 50% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0060 cm/cm | 0.0020 - 0.0060 in/in | ISO DIS 294-4 |
Wellman Wellamid® GFX1356-BK01 20% Glass Fiber Reinforced, Lubricated Nylon 6 Description: Glass Fiber Reinforced, Lubricated Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm | 0.0020 - 0.0040 in/in | on Tensile Bar; ISO 294 |
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | Eurotec |
Eurotec® Tecomid® NA43 GR25 NL XA43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, heat stabilized, natural, UL registered Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | ASTM D955 |
Clariant Renol PPSSP0006 Polyphenylene Sulfide, Glass Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | Eurotec |
Eurotec® Tecopet® PT70 KK45 PET, 45% glass fiber/mineral reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | ASTM and ISO value |
BASF Capron® 8234G 44% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8234G is a 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is .. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | Sheet |
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |