Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ISO 294-4 |
PolyOne LubriOne™ NN-30CF/15T-02S black Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne LubriOne™ PC-20CF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne LubriOne™ SF2-30CF/15T Natural Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne OnForce™ LFT UR-30 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ CTX-1125 Natural Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 3414R PC 40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0020 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LGK4030 PC (Asia Pacific) |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne Nymax™ GF 1200 60 HS Black 22 Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope.. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In.. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP 9X06030 PA 46 (Europe-Africa-Middle East) LNP* LUBRICOMP* 9X06030 is a compound based on PA46 resin containing PTFE and Carbon Fiber. Added features include: Internally Lubricated, Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0020 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | |
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PX5558 PPE+PS 30% glass reinforced, high flow PPO. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |
|||
Linear Mold Shrinkage, Flow | 0.00 - 0.0020 cm/cm @Thickness 3.18 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON DX09315C PC (Asia Pacific) LNP* Stat-Kon* DX09315C is carbon fiber filled polycarbonate composite with good flow ability, and high level of cleanliness for the most demanding application. A unique feature of this material is .. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP DC004E PC (Europe-Africa-Middle East) LNP* Thermocomp* DC004E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.00050 - 0.0020 cm/cm @Time 86400 sec |
0.00050 - 0.0020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific) LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WC006 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP RC003 PA 66 (Europe-Africa-Middle East) 15% carbon fibre reinforced Polyamide 66 injection moulding resin. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP RC003SXS PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC003SXS is a compound based on PA 66 resin containing Carbon fiber. Added features include: Electrically Conductive, Heat Stabilized |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; E2P method |
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; E2P method |
Eurostar Staramide PF00A PA6, 50% Glass Fiber Filled, Injection Molded Staramide PF00A is a 50% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | on Tensile Bar; E2P method |
Eurostar Staramide PF00AE PA6, 50% Glass Fiber Filled, Injection Molded Staramide PF00AE is a 50% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
Ravago Manufacturing Americas Hylex® P1310G40 HB Polycarbonate, 40% Fiberglass Reinforced, UV Stabilized Information provided by Ravago. |