Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Thermocomp* WC006 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 151 MPa
21900 psi
5 mm/min; ISO 527
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
5 mm/min; ISO 527
Flexural Strength 214 MPa
31000 psi
2 mm/min; ISO 178
Flexural Modulus 16.1 GPa
2340 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257