Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.028 - 0.032 cm/cm | 0.028 - 0.032 in/in | ASTM D955 |
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Linear Mold Shrinkage, Flow | 0.028 cm/cm @Time 86400 sec |
0.028 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Faradex KS003AI Acetal Copolymer (Europe-Africa-Middle East) LNP* FARADEX* KS003AI is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber. Added features include; EMI/RFI Shielding, Electrically Conductive.This data was supplied by SAB.. |
|||
Linear Mold Shrinkage, Flow | 0.028 cm/cm | 0.028 in/in | SABIC Method |
SABIC Innovative Plastics LNP STAT-LOY KX05015 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Loy* KX05015 is a compound based on Acetal Copolymer resin containing Antistat. Added features include permanent Anti-Static. |
|||
Linear Mold Shrinkage, Flow | 0.028 cm/cm | 0.028 in/in | SABIC Method |
SABIC Innovative Plastics LNP STAT-LOY KX09024 ACETAL COPOLYMER (Europe-Africa-Middle East) LNP* Statloy* KX09024 is a compound based on Polyacetal with reduced Resistivity. Added features include: Antistatic Properties |
|||
Linear Mold Shrinkage, Flow | 0.028 cm/cm | 0.028 in/in | SABIC Method |
SABIC Innovative Plastics LNP STAT-LOY KX01002 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Loy* KX01002 is a compound based on Acetal Copolymer resin containing Antistat. Added features include: Permanent Anti-Static. |
|||
Linear Mold Shrinkage, Flow | 0.028 cm/cm | 0.028 in/in | ISO 294-4 |
DSM EcoPaXX® Q-E7300 PA410-I Tube Extrusion |
|||
Linear Mold Shrinkage, Flow | 0.028 cm/cm | 0.028 in/in | ISO 294-4 |
DSM EcoPaXX® Q-X07207 PA410-I Impact Modified |
|||
Linear Mold Shrinkage, Flow | 0.028 cm/cm | 0.028 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.028 - 0.034 cm/cm @Thickness 4.00 mm |
0.028 - 0.034 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA66 D51 PA66, Injection Molded Star L PA66 D51 is a PTFE Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.028 - 0.034 cm/cm @Thickness 4.00 mm |
0.028 - 0.034 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L POM D74 POM, Injection Molded Star L POM D74 is a Proprietary Additive Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.028 cm/cm | 0.028 in/in | ISO 294-4 |
Barlog Plastics KEBAFLEX SG 45 A.1 TPE-S, Shore A45, natural TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Flow | 0.028 - 0.035 cm/cm @Time 86400 sec |
0.028 - 0.035 in/in @Time 24.0 hour |
|
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |