Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.021 cm/cm @Thickness 3.18 mm |
0.021 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Trilliant™ HC THC-02 1200 IL Natural Polyamide 66 (Nylon 66) The Trilliant® HC specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ah.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm @Thickness 2.00 mm |
0.021 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm @Thickness 2.00 mm |
0.021 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm @Thickness 2.00 mm |
0.021 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information pro.. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.024 cm/cm | 0.021 - 0.024 in/in | |
LATI Latilub 73/13-10ST POM, Silicone/PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). Silicone / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.029 cm/cm @Time 86400 sec |
0.021 - 0.029 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal LNP LUBRICOMP* KP004 is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.023 cm/cm | 0.021 - 0.023 in/in | SABIC Method |
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK (Europe-Africa-Middle East) LNP*LUBRICOMP* LFL36 is a compound based on Polyetheretherketone resin containing Glass Fiber, PTFE.
Added features include: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-A.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | SABIC Method |
SABIC Innovative Plastics LNP Lubricomp WL0049XF PBT LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant.This data was suppl.. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.027 cm/cm @Thickness 3.20 mm |
0.021 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.024 cm/cm @Thickness 3.20 mm |
0.021 - 0.024 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.024 cm/cm @Thickness 3.20 mm |
0.021 - 0.024 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V2000DM PBT (Europe-Africa-Middle East) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp MX96070 PP (Europe-Africa-Middle East) LNP* STARFLAM* MX96070 is a compound based on Polypropylene resin containing Flame Retardant. Added features include: Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP IP004Z PA6.12 (Europe-Africa-Middle East) LNP* LUBRICOMP* IP004Z is a compound based on PA 6/12 resin containing PTFE, Silicone. Added features include : Internally Lubricated, Extrusion grade. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP YI001 Polyester Elastomer (Europe-Africa-Middle East) LNP* LUBRICOMP* YI001 is a compound based on Polyester Elastomer containing Silicone. Added features include; Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | SABIC Method |
SABIC Innovative Plastics LNP STAT-KON KD000EI Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Kon* KD000EI is a compound based on Acetal Copolymer resin containing Carbon Powder. Added features include: Electrically Conductive, Impact Modified. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.027 cm/cm @Thickness 3.20 mm |
0.021 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ3001 PBT Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.024 cm/cm @Thickness 3.20 mm |
0.021 - 0.024 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V2000DM PBT Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | 0.125 in; ASTM D955 |
Chase Plastics CP Pryme® AH300 Acetal Homopolymer, Recycled Content Features: General purposeHigh heat resistanceGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGrease resistantLow moisture absorptionOil resistantHigh rigiditySolvent r.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AF is a high viscosity acetal homopolymer containing 20% Teflon PTFE fibers. It is designed for a.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO Data |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO 2577 |
BASF Ultraform® S2320 0035 LEV POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO 2577 |
BASF Ultraform® S2320 003 POM Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO 2577 |
BASF Ultraform® S2320 003 PRO POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm @Thickness 3.17 mm |
0.021 in/in @Thickness 0.125 in |
1/8" Section |