Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Asia Pacific) LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Asia Pacific) Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm .. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER (Asia Pacific) Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm .. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Asia Pacific) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and .. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm @Time 86400 sec |
0.0055 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER (Europe-Africa-Middle East) LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER (Asia Pacific) Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and .. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm @Thickness 3.20 mm |
0.0055 - 0.0075 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | Compression molding; ISO 2577 |
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
LATI Kelon® B FR H2 CE/25-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. Glass fibers. High impact resistance. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific;.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
LATI Latimass 82-03 D080 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
LATI Latishield 87/28-10A PC, Steel Fiber Reinforced EMI shielding product based on Polycarbonate (PC). Steel fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm @Time 86400 sec |
0.0055 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics NORYL WCP921 PPE-TPE Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain relief.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm @Thickness 3.17 mm |
0.0055 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF13 L BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm @Thickness 3.17 mm |
0.0055 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF14 HS L BK 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearan.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm @Thickness 3.17 mm |
0.0055 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF15 IM BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearan.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm @Thickness 3.17 mm |
0.0055 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF15 UV002 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: UV Stabilizer and LubricantFeatures: Good UV Resistance and LubricatedInforma.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | ISO 294-4 |
Styrolution Terlux® 2812 HD MABS Description: Terlux 2812 HD is a suitable grade for the food packaging and health care and diagnostic markets.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | |
BASF Polystyrol® 432 B Impact Grade Polystyrene (Europe) Very easy-flowing, low impact grade for parts with unfavorable flow path/wall-thickness ratios.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | |
BASF Polystyrol® 456 F Impact Grade Polystyrene (Europe) Heat distortion resistant, good flowing grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | |
BASF Polystyrol® 486 M Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H). Suitable for dairy packaging.Data was co.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | TM=300°C, TW=80°C |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Conditioned) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | 60x60x2 mm; ISO 294 |
BASF Ultradur® FRee B 4450 G5 LS 25% Glass Filled PBT Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so.. |