Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Stainless Steel Fiber
Manufacturer LATI
Trade Name Latishield
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latishield 87/28-10A PC, Steel Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
EMI shielding product based on Polycarbonate (PC). Steel fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm
0.0055 - 0.0075 in/in
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm
0.0060 - 0.0075 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
Elongation at Break 12 %
12 %
Tensile Modulus 3.10 GPa
450 ksi
Charpy Impact Unnotched NB
NB
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
Vicat Softening Point 145 °C

@Load 5.00 kg
293 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 300 ohm
300 ohm
Processing Properties Metric English Comments
Melt Temperature 265 - 300 °C
509 - 572 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Drying Temperature 110 - 130 °C
230 - 266 °F
Descriptive Properties Value Comments
Electromagnetic reflection 95 dB
ISO Shrinkage - Pressure 60 MPa