| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow |
0.0055
-
0.0075
cm/cm <br>@Thickness 3.20 mm
|
0.0055
-
0.0075
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER (Asia Pacific)
LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
-
0.0075
cm/cm <br>@Thickness 3.20 mm
|
0.0055
-
0.0075
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Asia Pacific)
Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
-
0.0075
cm/cm <br>@Thickness 3.20 mm
|
0.0055
-
0.0075
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Asia Pacific)
Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
-
0.0075
cm/cm <br>@Thickness 3.20 mm
|
0.0055
-
0.0075
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
-
0.0075
cm/cm <br>@Thickness 3.20 mm
|
0.0055
-
0.0075
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER (Asia Pacific)
Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
-
0.0075
cm/cm <br>@Thickness 3.20 mm
|
0.0055
-
0.0075
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
-
0.0075
cm/cm <br>@Thickness 3.20 mm
|
0.0055
-
0.0075
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Asia Pacific)
Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
-
0.0075
cm/cm <br>@Thickness 3.20 mm
|
0.0055
-
0.0075
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
|
|||
| Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | SABIC Method |
|
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific)
LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
cm/cm <br>@Time 86400 sec
|
0.0055
in/in <br>@Time 24.0 hour
|
ASTM D 955 |
|
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific)
LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
-
0.0075
cm/cm <br>@Thickness 3.20 mm
|
0.0055
-
0.0075
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® CFR9131 PC COPOLYMER (Asia Pacific)
Lexan* CFR9131 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and ..
|
|||
| Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | Test Condition: 60x60x2; 260°C / MT 80°C; 500 bar; ISO 294-4 |
|
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (Conditioned), Injection Molding Grade
Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage.
|
|||
| Linear Mold Shrinkage, Flow | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
|
LATI Latimass 82-03 D080 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
|
|||
| Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | |
|
LATI Latishield 87/28-10A PC, Steel Fiber Reinforced
EMI shielding product based on Polycarbonate (PC). Steel fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas..
|
|||
| Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | Compression molding; ISO 2577 |
|
Hexion Keripol® RZ 1141 Polyester Molding Compound, High Surface Quality
Polyester molding compound, organically/inorganically filled, glass fiber reinforced, styrene free, very slight post shrinkage, processing shrinkage as for phenolic molding compounds, high surface q..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
cm/cm <br>@Time 86400 sec
|
0.0055
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics NORYL WCP921 PPE-TPE
Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain relief..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
cm/cm <br>@Thickness 3.17 mm
|
0.0055
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES HiFill® PA6 GF15 L 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation ..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
cm/cm <br>@Thickness 3.17 mm
|
0.0055
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES HiFill® PA6 GF15 L BK 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackProcessing Method: Injection Mo..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
cm/cm <br>@Thickness 3.17 mm
|
0.0055
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES HiFill® PA6 GF15 UV002 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: UV Stabilizer and LubricantFeatures: Good UV Resistance and LubricatedInforma..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
-
0.0065
cm/cm <br>@Thickness 3.20 mm
|
0.0055
-
0.0065
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Noryl GTX GTX8710 PPE+PA
Noryl GTX8710 resin is a glass filled, high performance blend of PPE/PA that exhibits an exceptional balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-sta..
|
|||
| Linear Mold Shrinkage, Flow | 0.0055 - 0.0075 cm/cm | 0.0055 - 0.0075 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS
PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers.
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
-
0.0075
cm/cm <br>@Thickness 3.00 mm
|
0.0055
-
0.0075
in/in <br>@Thickness 0.118 in
|
150x105x3mm; b.o. ISO 2577 |
|
Covestro Bayblend® M850 XF PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Eas..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
-
0.0075
cm/cm <br>@Thickness 3.00 mm
|
0.0055
-
0.0075
in/in <br>@Thickness 0.118 in
|
150x105x3mm; b.o. ISO 2577 |
|
Covestro Bayblend® T80 XG PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Opt..
|
|||
| Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | |
|
BASF Polystyrol® 445 E WU Impact Grade Polystyrene (Europe)
Easy flowing, heat-resistant, medium-impact, flame-retardant grade. Application example: electrical distribution boxes.Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | |
|
BASF Polystyrol® 476 L Impact Grade Polystyrene (Europe)
Normal flowing, high-impact grade. When extruded it is often mixed with PS 165 H.Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | |
|
BASF Polystyrol® 585 K Impact Grade Polystyrene (Europe)
Special high gloss, high-impact grade for all types of housings. Basis product for gloss capping.Data was collected by ISO methods and provided by BASF.
|
|||
| Linear Mold Shrinkage, Flow | 0.0055 cm/cm | 0.0055 in/in | TM=300°C, TW=80°C |
|
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry)
Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
-
0.0075
cm/cm <br>@Thickness 3.20 mm
|
0.0055
-
0.0075
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Asia Pacific)
Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
|
|||
| Linear Mold Shrinkage, Flow | 0.0055 - 0.0085 cm/cm | 0.0055 - 0.0085 in/in | |
|
LATI Latimass 82-03 D110 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
|
|||
| Linear Mold Shrinkage, Flow |
0.0055
cm/cm <br>@Thickness 3.17 mm
|
0.0055
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Techmer ES Luriblend® POM CO GF20 TL20 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE LubricantFeatures: Lubricated and CopolymerInformation provided by TP Composites, Inc.
|
|||