Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z300 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z300 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z400 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z400 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z500 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z600 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z600P Thermoplastic Elastomer, SEBS-based, Co-injection, PA-adhesion Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z650A Thermoplastic Elastomer, SEBS-based, Co-injection Grade Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z700 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z700 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z800 SHF Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z800 SHF Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z800 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z800 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z900 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE Z900 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.014 - 0.024 cm/cm | 0.014 - 0.024 in/in | FRISETTA Test Method |
Nilit RECONYL A H Recycled nylon 6.6 for injection molding Recycled nylon 6.6 for injection molding, heat stabilized (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.014 - 0.024 cm/cm | 0.014 - 0.024 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 H Nylon 6.6 for injection molding Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.014 - 0.024 cm/cm | 0.014 - 0.024 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 HH Nylon 6.6 for injection molding Nylon 6.6 for injection molding, heat and hydrolysis stabilizedInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.016 - 0.024 cm/cm | 0.016 - 0.024 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 D Nylon 6., std. viscosity for injection molding Nylon 6., std. viscosity for injection molding, permanently flexible, developed for dowels.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | |
Lehmann & Voss LUVOCOM® 80-8387/EM Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, .. |
|||
Linear Mold Shrinkage | 0.014 - 0.024 cm/cm | 0.014 - 0.024 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 2890 Thermoplastic Elastomer Elastocon® 2890 thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2890 is FDA compliant and well suited for cons.. |