| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | With Flow; ISO 2577 |
| 0.017 - 0.024 cm/cm | 0.017 - 0.024 in/in | Across Flow; ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 90 @Time 15.0 sec |
90 @Time 0.00417 hour |
Polykemi |
| Tensile Strength at Break | <= 14.0 MPa | <= 2030 psi | ISO/R527 |
| Elongation at Break | 450 % | 450 % | ISO/R527 |
| 100% Modulus | 0.00450 GPa | 0.653 ksi | ISO/R527 |
| 300% Modulus | 0.00620 GPa | 0.899 ksi | ISO/R527 |
| Tear Strength | 45.0 kN/m | 257 pli | D624 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
| Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
| Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure () | Low | % of injection pressure |
| Injection Pressure | Low | |
| Injection Speed () | High |