Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00600 - 0.00900 cm/cm @Temperature 80.0 - 121 °C |
0.00600 - 0.00900 in/in @Temperature 176 - 250 °F |
Average value: 0.00750 cm/cm Grade Count:3 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.00600 - 0.00900 cm/cm @Time 3600 - 3600 sec |
0.00600 - 0.00900 in/in @Time 1.00 - 1.00 hour |
Average value: 0.00750 cm/cm Grade Count:3 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00900 cm/cm | 0.000 - 0.00900 in/in | Average value: 0.00184 cm/cm Grade Count:17 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00900 cm/cm | 0.00100 - 0.00900 in/in | Average value: 0.00291 cm/cm Grade Count:52 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00900 cm/cm | 0.00200 - 0.00900 in/in | Average value: 0.00508 cm/cm Grade Count:111 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00900 cm/cm | 0.00100 - 0.00900 in/in | Average value: 0.00321 cm/cm Grade Count:56 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00900 cm/cm | 0.00100 - 0.00900 in/in | Average value: 0.00256 cm/cm Grade Count:72 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00900 cm/cm | 0.00100 - 0.00900 in/in | Average value: 0.00177 cm/cm Grade Count:44 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00900 cm/cm | 0.00300 - 0.00900 in/in | Average value: 0.00517 cm/cm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00900 cm/cm | 0.00200 - 0.00900 in/in | Average value: 0.00655 cm/cm Grade Count:33 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00900 cm/cm | 0.00100 - 0.00900 in/in | Average value: 0.00700 cm/cm Grade Count:14 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Linear Mold Shrinkage | 0.000200 - 0.00900 cm/cm | 0.000200 - 0.00900 in/in | Average value: 0.00341 cm/cm Grade Count:110 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00900 cm/cm | 0.00300 - 0.00900 in/in | Average value: 0.00557 cm/cm Grade Count:55 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage | 0.00281 - 0.00900 cm/cm | 0.00281 - 0.00900 in/in | Average value: 0.00522 cm/cm Grade Count:21 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00900 cm/cm | 0.000500 - 0.00900 in/in | Average value: 0.00262 cm/cm Grade Count:34 |
Overview of materials for Nylon 612, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00900 cm/cm | 0.00300 - 0.00900 in/in | Average value: 0.00639 cm/cm Grade Count:25 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00900 cm/cm | 0.00200 - 0.00900 in/in | Average value: 0.00491 cm/cm Grade Count:7 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage | 0.00600 - 0.00900 cm/cm @Temperature 80.0 - 121 °C |
0.00600 - 0.00900 in/in @Temperature 176 - 250 °F |
Average value: 0.00750 cm/cm Grade Count:1 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Linear Mold Shrinkage | 0.00600 - 0.00900 cm/cm @Time 3600 - 3600 sec |
0.00600 - 0.00900 in/in @Time 1.00 - 1.00 hour |
Average value: 0.00750 cm/cm Grade Count:1 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00900 cm/cm | 0.00300 - 0.00900 in/in | Average value: 0.00600 cm/cm Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00900 cm/cm | 0.00400 - 0.00900 in/in | Average value: 0.00580 cm/cm Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |