Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | |
Plastcom SLOVALEN PH 66 GF 20 FRO 4 PP, 20% glass fibre, flame retardant FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre, with decreased flammability. Used in the electrical industry - teroderately increased toughness an.. |
|||
Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | |
Plastcom SLOVAMID 6 NGR PA6, basic type FeaturesPA 6 for injection moulding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, faste.. |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | With Flow; ISO 2577 |
Polykemi AB POLYform POM C M140 Polyoxymethylene Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | With Flow; ISO 2577 |
Polykemi AB POLYshine PBT D201 PBT Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYshine PBT D241 PBT, Impact Modified Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | With Flow; ISO 2577 |
Polykemi AB POLYform POM C M90 Polyoxymethylene Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | Asahi Chemical test |
Asahi Kasei Tenac® GT525 Acetal Homopolymer, 25% Glass Beads
(discontinued **) 25% glass beads-filled grade with superior isotropic dimensional stability.Applications: Speedometer frames.This product is not a part of the standard product line dated 2003. |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | |
Custom Resins Duratel™ MF3 Acetal Copolymer
(discontinued **) Description: Duratel™ MF3 is a 2.5 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL N109-HR Heat Resistant POM, Unreinforced, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL N127-AS Antistatic POM, Unreinforced, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL VC-145 Antistatic POM, Unreinforced, Ultra High Flow, For VCR Reels LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 - 0.019 cm/cm | 0.018 - 0.019 in/in | ASTM D955 |
Kolon KOPA® KN170SA General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | |
Polyram RamTal PM7013 Acetal, UV Stabilized Polyacetal copolymer UV stabilized for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | |
Polyram RamTal RM7009 Acetal, UV Stabilized UV stabilized acetal copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | |
Polyram RamTal PM1609 Acetal, Molybdenum Disulfide Filled Molybdenum disulfide filled polyacetal for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.018 - 0.026 cm/cm @Thickness 3.20 mm |
0.018 - 0.026 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 395 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | ASTM D955 |
Cheng Yu Plastic SW02 POM/PTFE |
|||
Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | ASTM D955 |
Cheng Yu Plastic SW10 POM/PTFE |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | |
CPT C-Flex® R70-089 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Linear Mold Shrinkage | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47 Nylon 66, Conditioned Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st.. |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | Asahi Kasei Method |
Asahi Kasei Tenac® LA543 Homopolymer Acetal Resin Excellent friction and wear on metals and plastics, except POM.Information provided by Asahi Kasei Corporation. |
|||
Linear Mold Shrinkage | 0.018 cm/cm | 0.018 in/in | STN 64 0808 |
Plastcom SLOVALEN PQ 51 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Linear Mold Shrinkage | 0.018 - 0.022 cm/cm | 0.018 - 0.022 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® ESD 12-000
(discontinued **) PRE-ELEC ESD 12-000 is a static dissipative thermoplastic compound based on polyacetal copolymer. The dissipative property is permanent and built into the polymer chain. The products made out of PRE.. |