Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | |
NYCOA 1838 Copolymer Nylon Alloy good impact resistant molding and extrusion gradeInformation provided by NYCOA, Inc. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | |
NYCOA 578 PA 6 very high viscosity molding & extrusion grade for tubing, pipes, film and tapesInformation provided by NYCOA, Inc. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Network Polymers Nylon 6609 L Description: Black NylonInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | 4 mm thick, 10.0 mm wide molded rod; ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PE 1291 PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm @Thickness 4.00 mm |
0.015 - 0.025 in/in @Thickness 0.157 in |
10.0 mm wide molded rod; ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | With Flow; ISO 2577 |
Polykemi AB SCANAMID 66 A32^E Nylon 66, Modified Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANCOMP PP BN140 T5 Polypropylene Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.015 - 0.022 cm/cm | 0.015 - 0.022 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 AV15 Nylon 6.6 for injection molding Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | |
Lehmann & Voss LUVOCOM® 1-7968 Polyamide 66, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Dynamic stressed parts.Isotrop.. |
|||
Linear Mold Shrinkage | 0.015 - 0.021 cm/cm | 0.015 - 0.021 in/in | |
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Linear Mold Shrinkage | 0.015 - 0.017 cm/cm | 0.015 - 0.017 in/in | ASTM D1299 |
Loxim 810 02T HB Polypropylene Compound, 10% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Linear Mold Shrinkage | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
|
Shakespeare Isocorâ„¢ HZ73SI high viscosity PA-6 Isocorâ„¢ HZ73SI is a high viscosity PA-6. This resin is specifically suited for applications requiring excellent abrasion, tensile and elongation properties. This resin can be processed using.. |
|||
Linear Mold Shrinkage | 0.015 - 0.022 cm/cm | 0.015 - 0.022 in/in | ASTM D955 |
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Teknor Apex Monprene® MP-1473 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Teknor Apex Monprene® MP-1479 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm @Thickness 3.175 mm |
0.015 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Tipco Tipcolene® FPT 10 - 10% Talc Reinforced Polypropylene Homopolymer 10% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Linear Mold Shrinkage | 0.015 cm/cm @Thickness 3.175 mm |
0.015 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6 Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | ASTM D955 |
A. Schulman POLYFLAM™ RPP 1058 General Purpose Homopolymer Polypropylene (30% Fiberglass) DescriptionPolyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Sch.. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | ASTM D 955 |
Cossa Polimeri ESTAPROP 1000 V2 K Flame Retardant Polypropylene PP copolymerFlame retardant class V2, PBDE free, good processability, good impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | |
E-Polymers TEKAMID® TA210 LW TA210LW, Low Wear, Low Friction PA66, DAM Low wear, Low frictionInformation provided by E-Polymers Co. Ltd. |
|||
Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 51 T 15 Polypropylene Homopolymer, 15% Mineral Filled FeaturesModified homopolymer PP for injection moulding with the content of 15% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application .. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | 0.125; ASTM D955 |
LTL Color Compounds ColorFast® NY2 Nylon 66 Nylon 6,6 with or without lubeAll information provided by LTL Color Compounders, Inc. |