Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM D955-89 |
Multibase Multi-Flex® TPO D-6403 Multi-Flex® D 6403 is a rubber modified polypropylene compound for automotive applications such as bumper-covers, step in pads, rubstrips, and airdams.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM D955 |
Multibase Multi-Pro® 4017 C Polypropylene Calcium Carbonate Filler, 40% by weight.Features:Stiffness, Good Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Linear Mold Shrinkage | 0.010 - 0.030 cm/cm | 0.010 - 0.030 in/in | |
Multibase TPSiV® 4200-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | |
Nylene® PA6/6 Mineral Filled 6140 HS Nylon 6/6 40% Mineral Filler; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | ASTM D955 |
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH T20020 UV Polypropylene Homopolymer, Mineral Reinforced, UV-Stabilized Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Acctuf® 3243 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-8319 PEEK, with PTFE, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM D995 |
Huntsman IROGRAN® A 92 K 5031 TPU-High Temperature Performance Polycaprolactone and ether based. Good processability and compression set. Excellent resistance to high temperatures, water, grease, and oils.. Used in seals, wheels, and rollers.Information prov.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
Ineos H01G-00 Polypropylene Homopolymer Grade H01G-00 is a polypropylene homopolymer for fiber, tape, and consumer applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.152.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM D955 |
Multibase Multi-Flex® G 7940 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good General PurposeOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInfor.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-7018/GN PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
Teknor Apex Flexalloy® 9300-70 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | Isotropy |
Solvay TECHNYL® C 536XT PA6, DRY Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM D955 |
Teknor Apex Sinpolene CPP2020 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 20% Filler by Weight Features: Copolymer Uses: Furniture Forms: PelletsInformation Provided .. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
Borealis BF330MO Polypropylene Copolymer BF330MO is a heterophasic copolymer. This polymer is characterized by an optimum combination of high stiffness, high impact strength and good flow properties. This grade is designed for high-speed i.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | average process; cross flow; 150x80x2mm |
Borealis GB311U Polypropylene Compound, Glass Fiber Reinforced GB311U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
Borealis RG460MO Polypropylene, Transparent Random Copolymer RG460MO is a specially modified transparent polypropylene random copolymer with high melt flow. and is designed for high-speed injection molding and contains nucleating and demolding additives. Pro.. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
Borealis RJ370MO Polypropylene, Transparent Random Copolymer RJ370MO is a specially modified highly-transparent polypropylene random copolymer with very high melt flow rate. It is designed for high-speed injection molding and contains nucleating and demoldin.. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | |
Borealis Borpact™ SE920MO Polypropylene Homopolymer for Injection Molding Borpact SE920MO is a high impact and transparent polypropylene. Borpact SE920MO is a new generation polypropylene having properties that were earlier not possible to combine. Borpact SE920MO offers.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm @Thickness 3.175 mm |
0.010 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULAMID® 6 GF15H 15% Glass Bead Reinforced, Heat Stabilized Nylon 6 Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | |
Cytec EN-9 (OZR) (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Homopolymer HP0334T30L Talc Reinforced |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM Data; MD |
BASF Ultramid® C33 01 PA66/6 (Conditioned) Ultramid C33 01 is an intermediate viscosity PA6/66 grade. Its lower melting point than standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It conforms to F.. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPHC T8020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Acclear® 8449 Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Good impact, Excellent static controlTypical applications: Housewares, Rigid packagingComplies wit.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Amoco® Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection molding; Rotary CompressionFeatures: Nucleated, Antistatic, LubricatedTypical applications: Closures, CapsComplies with FDA specification, Title 21, CFR 177... |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Acctuf® 3434 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High gloss, Nucleated, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded s.. |