Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
RheTech Products FT7012-707UV Thermoplastic Polyolefin, UV Stabilized, 848 Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 GF 30 LS Polyamide 6, 30% Glass Fiber, UV Stabilization FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools... |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Oxford Polymers 10GF 10% Glass Fiber Reinforced Polyetherimide/Polycarbonate Alloy 10% Glass Fiber Reinforced Polyetherimide/Polycarbonate AlloyInformation provided by Oxford Polymers. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | Isotropy |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Spartech Royalite R21M General Purpose ABS Resin Data provided by the manufacturer. A general-purpose ABS resin with high impact strength, R-21M is a popular choice for a variety of products, from bicycle helmets and carrying cases to portable ta.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM Data; MD |
Styrolution Luran® S 777 K ASA Luran S 777 K is an easy flowing injection molding ASA grade with good toughness and heat distorsion resistance. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM Data; MD |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM Data; MD |
Styrolution Terlux® 2812 TR MABS Terlux 2812 TR is a transparent grade of MABS for injection molding with high flowability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 2620 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 348 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 545 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 555 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 9030 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ SPD 214 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 341 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Tipco Tipcolite® TMS 211 Phenolic Compound, Cotton, Filler & Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Cotton, Filler & Wood FlourApplications: Industrial & AutomotivesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | Bayer Test |
Covestro Bayflex® 180 Polyurethane Elastomeric RIM, 20% Mica Filled, MDI-based 2-Component Liquid System 0.150 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Dow AIM® 4810 High Impact Styrenic Resin AIM® 4810 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Dow AIM® 4900 High Impact Styrenic Resin AIM® 4900 advanced styrenic resin for extrusion and thermoforming applications is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Adell AR-33 Nylon 66, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Adell AT-14 Nylon 66, 20% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Adell BT-34 Nylon 6, 20% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Conditioned) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
BASF Ultramid® A3WG5 25% Glass Filled PA66 (Conditioned) Ultramid A3WG5 is a 25% glass fiber reinforced and heat resistance injection molding PA66 grade. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | restricted |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | restricted |
BASF Ultramid® B3S BK00464 PA6 (Conditioned) Description: Easy flowing, finely crystalline injection-molding grade for very fast processing. Uses include thin-walled technical parts (eg. housings, fittings, grips, small parts and fixing clamps.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | LATI |
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)
(discontinued **) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 9020 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 9025 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |