Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00100 - 0.00200 cm/cm | 0.00100 - 0.00200 in/in | ASTM D955 |
Niche Polymer PPHT20BK Homopolymer PP, 20% Talc Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.00652 cm/cm Grade Count:92 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00599 cm/cm Grade Count:49 |
Overview of materials for Polyphenylene Ether, Heat Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00200 cm/cm | 0.00100 - 0.00200 in/in | Average value: 0.00144 cm/cm Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00700 cm/cm | 0.00100 - 0.00700 in/in | Average value: 0.00505 cm/cm Grade Count:5 |
Overview of materials for Polyphenylene Ether, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00289 cm/cm Grade Count:35 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00514 cm/cm Grade Count:131 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00600 cm/cm | 0.00100 - 0.00600 in/in | Average value: 0.00277 cm/cm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00900 cm/cm | 0.00100 - 0.00900 in/in | Average value: 0.00177 cm/cm Grade Count:44 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0140 cm/cm | 0.00100 - 0.0140 in/in | Average value: 0.00636 cm/cm Grade Count:17 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00700 cm/cm | 0.00100 - 0.00700 in/in | Average value: 0.00443 cm/cm Grade Count:7 |
Overview of materials for Polycarbonate, Foam Grade, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00325 cm/cm Grade Count:12 |
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Linear Mold Shrinkage | 0.00100 cm/cm | 0.00100 in/in | Average value: 0.00100 cm/cm Grade Count:3 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00319 cm/cm Grade Count:7 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0350 cm/cm | 0.00100 - 0.0350 in/in | Average value: 0.0300 cm/cm Grade Count:123 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0550 cm/cm | 0.00100 - 0.0550 in/in | Average value: 0.00760 cm/cm Grade Count:191 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0180 cm/cm | 0.00100 - 0.0180 in/in | Average value: 0.00481 cm/cm Grade Count:51 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0300 cm/cm | 0.00100 - 0.0300 in/in | Average value: 0.00469 cm/cm Grade Count:144 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00288 cm/cm Grade Count:3 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00313 cm/cm Grade Count:9 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0160 cm/cm | 0.00100 - 0.0160 in/in | Average value: 0.00673 cm/cm Grade Count:70 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0500 cm/cm | 0.00100 - 0.0500 in/in | Average value: 0.00570 cm/cm Grade Count:30 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00429 cm/cm Grade Count:12 |
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00400 cm/cm | 0.00100 - 0.00400 in/in | Average value: 0.00240 cm/cm Grade Count:5 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.0117 cm/cm Grade Count:27 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.00629 cm/cm Grade Count:115 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.00511 cm/cm Grade Count:287 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0100 cm/cm | 0.00100 - 0.0100 in/in | Average value: 0.00374 cm/cm Grade Count:45 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0170 cm/cm | 0.00100 - 0.0170 in/in | Average value: 0.00851 cm/cm Grade Count:16 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |