Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.017 - 0.023 cm/cm | 0.017 - 0.023 in/in | ASTM D955 |
Kolon SPESIN® KP210 General Purpose PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Linear Mold Shrinkage | 0.011 - 0.023 cm/cm | 0.011 - 0.023 in/in | FRISETTA Test Method |
Nilit FRIANYL C73 S10 Nylon 6.6/6 for injection molding Nylon 6.6/6 for injection molding, medium viscosity, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.0040 - 0.023 cm/cm | 0.0040 - 0.023 in/in | FRISETTA Test Method |
Nilit RECONYL A GV30 Recycled nylon 6.6 for injection molding, 30% glass fiber reinforced Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | ASTM D955 |
PolyOne Lubri-Tech™ AT-000/20T Copolymer Acetal - 20% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.021 - 0.023 cm/cm | 0.021 - 0.023 in/in | ASTM D955 |
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Linear Mold Shrinkage | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ASTM D955 |
Kolon KOPA® KN333HFBL General Purpose Nylon 66 Middle viscosity, flexibleApplications Band cables for vehiclesInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.017 - 0.023 cm/cm | 0.017 - 0.023 in/in | ASTM D955 |
Kolon SPESIN® KP211 General Purpose PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Linear Mold Shrinkage | 0.017 - 0.023 cm/cm | 0.017 - 0.023 in/in | ASTM D955 |
Kolon SPESIN® KP270 General Purpose PBT Base Resin Excellent extrudabilityApplications: CablesInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.018 - 0.023 cm/cm | 0.018 - 0.023 in/in | ASTM D955 |
Kolon SPESIN® KP270BL General Purpose PBT Compound Resin Excellent waterproofnessApplications: ConnectorsInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.017 - 0.023 cm/cm | 0.017 - 0.023 in/in | ASTM D1299 |
Loxim 200 00HB Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Linear Mold Shrinkage | 0.017 - 0.023 cm/cm | 0.017 - 0.023 in/in | ASTM D1299 |
Loxim 200 00V0 Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Linear Mold Shrinkage | 0.017 - 0.023 cm/cm | 0.017 - 0.023 in/in | ASTM D1299 |
Loxim 800 00 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Linear Mold Shrinkage | 0.015 - 0.023 cm/cm | 0.015 - 0.023 in/in | 0.125; ASTM D955 |
LTL Color Compounds ColorFast® FRPBT200 PBT, Flame Retarded V-0 rated, unfilled PBTAll information provided by LTL Color Compounders, Inc. |
|||
Linear Mold Shrinkage | 0.015 - 0.023 cm/cm | 0.015 - 0.023 in/in | 0.125; ASTM D955 |
LTL Color Compounds ColorFast® PBT100 PBT General purpose injection molding grade unfilled PBT with lubeAll information provided by LTL Color Compounders, Inc. |
|||
Linear Mold Shrinkage | 0.014 - 0.023 cm/cm @Thickness 3.00 mm |
0.014 - 0.023 in/in @Thickness 0.118 in |
ASTM D955 |
Samyang Tribit® 1500 Polybutylene Terephthalate Characteristics:Medium viscosityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samy.. |
|||
Linear Mold Shrinkage | 0.014 - 0.023 cm/cm | 0.014 - 0.023 in/in | ASTM D955 |
Samyang Tribit® 1510 PBT, Middle Viscosity Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1510 is a middle viscosity grade.Informatio.. |
|||
Linear Mold Shrinkage | 0.014 - 0.023 cm/cm | 0.014 - 0.023 in/in | ASTM D955 |
Samyang Tribit® 1700 PBT, Middle Viscosity Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1700 is a middle viscosity grade.Informatio.. |
|||
Linear Mold Shrinkage | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ISO 294-4 |
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Linear Mold Shrinkage | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | |
Polyram RamTal PM8427 Acetal, Impact modified Impact modified polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.021 - 0.023 cm/cm | 0.021 - 0.023 in/in | ISO 2577 |
Polyram RamSter PF810 PBT, Impact Modified Impact modified PBT for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | |
Polyram RamTal PM8515 Acetal, High impact High impact polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.014 - 0.023 cm/cm | 0.014 - 0.023 in/in | ASTM D955 |
Samyang Tribit® 1800 PBT, High Viscosity Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1800 is a high viscosity grade.Information .. |
|||
Linear Mold Shrinkage | 0.014 - 0.023 cm/cm | 0.014 - 0.023 in/in | ASTM D955 |
Samyang Tribit® 1800H PBT, Extruding Formality Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1800H is an extrusion grade.Information pro.. |