Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0050 - 0.010 cm/cm | 0.0050 - 0.010 in/in | (longitudinal) Compression; ISO 2577 |
Raschig Group MELOPLAS® 150 MF Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr.. |
|||
Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | 0.125 in, DAM; ASTM D955 |
Ravago Manufacturing Americas Hylon® N1040ML Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH T2040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | |
Lehmann & Voss LUVOCOM® 1105-8382 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Highly dimensionally stable at ele.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | ASTM D955 |
Kolon KOLEFIN® KO133MT40 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | ASTM D955 |
Kolon SPESIN® KP213G20WBL Glass Fiber Reinforced & Weather Resistant PBT Compound Resin G/F 20% reinforced, weather resistanceApplications: Parts of electric lightInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.0030 - 0.010 cm/cm | 0.0030 - 0.010 in/in | ASTM D955 |
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.0050 - 0.010 cm/cm | 0.0050 - 0.010 in/in | |
Lehmann & Voss LUVOCOM® 1105-7023/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | ASTM D955 |
Teknor Apex Chemlon® 240 MH Nylon 6, 40% Short Glass Fiber Reinforced Features: Heat Stabilized; Warp Resistant Forms: Pellets Additive: Heat Stabilizer Automotive Specifications: GM GMP.PA6.011Information Provided by Teknor Apex |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm @Thickness 3.20 mm |
0.0080 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | as molded |
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.010 cm/cm @Thickness 3.175 mm |
0.0030 - 0.010 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66 Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm |
0.0060 - 0.010 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0060 - 0.010 in/in @Thickness 0.126 in, Time 72.0 hour |
ISO 294 |
A. Schulman FORMION™ FI 243 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0060 - 0.010 in/in @Thickness 0.126 in, Time 72.0 hour |
ISO 294 |
A. Schulman FORMION™ FI 372 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | as molded |
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i.. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | ASTM D 955 |
Cossa Polimeri ESTAPROP H 10100 BS Polypropylene, 50% Mineral Filled PP homopolymer 50% mineral fillerExcellent surface appearance, high densityInformation provided by Cossa Polimeri S.r.l. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | |
Ecomass® 1850ZN66T1 Steel Powder Filled Polyamide, Injection Molding Steel Powder Filled Polyamide (PA6), Impact Modified, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInformation provide.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | ASTM D955 |
Ecomass® 3608TU96 Tungsten Filled Polyethylene Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyethylene (HDPE)Information provided by Technical Polymers |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm @Thickness 4.00 mm |
0.0080 - 0.010 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000 GS 50 HWUVCP 50% Glass Sphere Filled Nylon 6, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | ASTM D955 |
Diamond Polymers ASA TWP 121 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH T5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in | ASTM D955 |
Asahi Kasei Xyron® X9108 Modified Polyphenylene Ether High-Heat ResistantInformation provided by Asahi Kasei |
|||
Linear Mold Shrinkage | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | |
Polyram RamOfin PPC359T4 Polypropylene, 20% Mineral Filled 20% mineral filled, heat stabilized and impact modified for polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |