Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm @Thickness 3.17 mm |
0.0050 - 0.0080 in/in @Thickness 0.125 in |
|
Ovation Polymers Opnyl OP66GF15 Nylon 66, 14% Glass Reinforced Nylon 66 - Glass reinforced (14 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Network Polymers NPP 808 C2WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYblend 85VB PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANBLEND FS8 FR UV PC/ASA, Flame Retardant, UV-Stabilized Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | Across Flow; ISO 2577 |
Polykemi AB SCANBLEND SS7 PC/ASA, UV-Resistant Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PC-GP2-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Medium Flow Polycarbonate, FDA-compliant Feedstocks, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized Polycarbonate, Impact Modified, Low Flow, UV-stabilizedProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PPX-FR2-[color]EN Modified PPO, UL 94 V-1 with HDT of 210 F, Extrusion Grade Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | as molded; ISO 294 |
Solvay Engineered Polymers SEQUEL® 1440LS TPO
(discontinued **) Description: SEQUEL® 1440LS engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent processabilit.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PPX-GP2 Modified PPO, General Purpose with HDT of 250 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | ASTM D955 |
Alcoa KAMA 3400 Super High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm @Temperature 23.0 °C |
0.0050 - 0.0070 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa JH960 HT10 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | ASTM D955 |
Global NPP-130-C Glass/Talc Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm @Temperature 23.0 °C |
0.0050 - 0.0070 in/in @Temperature 73.4 °F |
ASTM D955 |
Kingfa MAC-451 UV Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Kolon KOPA® KN133G30 G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | ASTM D955-89 |
Multibase Multi-ABS 801 Natural Extrusion Grade Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Samyang Trirex® 3026PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3026PJ is an extrusion grade.Information provided by Samyang. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | |
Polyram RamLloy PBB104 PC/ABS alloy, Injection Molding PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in | |
Polyram RamLloy PJ701 ABS/ASA, General Purpose PJ 701 IS A GENERAL PURPOSE INJECTION MOLDING ASA& ABS ALLOY . IT HAS GOOD MECHANICAL PROPERTIES SIMILAR TO ABS AND MUCH BETTER WEATHER RESISTANCE. AN IDEAL ECONOMIC CHOICE.Information provided .. |
|||
Linear Mold Shrinkage | 0.0050 cm/cm @Thickness 3.175 mm |
0.0050 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman ComAlloy® E-12672 Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D 955 |
Cossa Polimeri ESTACARB 2060 V0 Flame Retardant Polycarbonate Flame retardant class V0, antimony and PBDE free, opaque, high melt flow, high impact strength, high thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Asahi Kasei Xyron® 300Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Aaron Industries AAROPRENE® AEPC 5000-1 Engineered Polycarbonate Resin Melt flow index may be specified. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | |
E-Polymers TEKALOY® G75NHT Brominated Flame Retardant High Impact PC/ABS Alloy PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan.. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
Polymer Resources PPX-GP6 Modified PPO, General Purpose with HDT of 290 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |