Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955-89 |
Multibase Multi-Pro® 4003 RC 40% Glass Filled Polypropylene Multi-Pro 4003 RC is a chemically coupled glass reinforced polypropylene compound suitable for engineered plastics applications due to its high heat, flexural and impact properties.Data provided by .. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | Measured on a tensile specimen.; ISO 294-4 |
PolyOne OnForce™ LFT NN-40LCF/001 Grey Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | With Flow; ISO 2577 |
Polykemi AB SCANMID 6 B12^ F20 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0030 - 0.0080 cm/cm | 0.0030 - 0.0080 in/in | |
Lehmann & Voss LUVOCOM® 19-7912 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Gear parts f.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | |
Lehmann & Voss LUVOCOM® 21-7928 Polyamide 6/6T, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
KKPC Kuhmo HI 450S High Gloss HIPS Key features: High-gloss Common Uses: Portable CD-case, air conditioner cases.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impac.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | |
Lehmann & Voss LUVOCOM® 1105-0779/WT PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High chemical resistance parts, hydrolysis resistance, non flammable.H.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
KKPC Kuhmo HI 425EP Extrusion Molding HIPS Common Uses: Refrigerator inner liners, door liners, disposable cups, food packaging sheet, wrapping films, trays, washing machinesHIPS is a functional resin made by copolymerization of styrene mono.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | Compression Molding; ASTM D955 |
Sumitomo Bakelite North America E 8940SG Electrical Encapsulation Grade Epoxy Mineral reinforced epoxy molding compound formulated for the encapsulation of electronic devices requiring high quality, exceptional reliability, and outstanding moldability. USES: Passive electron.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | |
Videolar 500 Crystal Polystyrene (GPPS) Designed for injection moldingVery easy flowing grade for fast cycle injection moldingExcellent processability for filling thin partsFeatures: Good strengthGood temperature resistanceExcellent clari.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ISO 2577 |
Polyram PlusTek RA303G33 Nylon 66 for Injection Molding, 33% Glass Fiber Reinforced, Heat Stabilized, Hydrolysis Resistant 33% Glass fiber reinforced, heat stabilized and hydrolysis resistant Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm @Thickness 3.175 mm |
0.0030 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D 955 |
Cossa Polimeri ESTADIENE 1030 T V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high thermal resistance, good impact resistance, high gloss, good light resistance, good processabilityInformation provided by Cos.. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm @Thickness 4.00 mm |
0.0030 in/in @Thickness 0.157 in |
|
CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | |
Eurotec® Tecomid® NA40 GR25 NL PA 6.6 25% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM Data; MD |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM Data; MD |
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Conditioned) Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, heat stabilized, impact modified, pigmented black, PA6 injection molding compound developed for applications requiring improved dry as molded t.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0090 cm/cm | 0.0030 - 0.0090 in/in | ASTM D955 |
Beijing Ranger Chem PBT-201-G30 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
Adell ZR-37 33% Glass Reinforced Nylon/Olefin Alloy Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | |
BASF Ultramid® B3WG6 HP BK 23210 30% Glass Filled PA6 (Conditioned) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade with enhances flowability used e.g. for automobile manifold.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | Injection Molding; ISO 2577 |
Vyncolit X611 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Complex precision parts with thin cross section and good mechanical properties e.g. in.. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | |
Eurotec® Tecodur® PB70 GR45 NL PBT 45% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
Sumitomo Bakelite North America FM 7700P Fiberglass and Mineral Reinforced Phenolic Novolac FM 7700P is a two-stage phenolic molding compound reinforced with cotton fabric in pellet form. FM-7700P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-20. (Replaces Mil.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ASTM D955 |
PolyOne Edgetek® PI-10CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedElectrically ConductiveInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
PlastxWorld DAICEL STYROL® GW50 HIPS UV stable flame retarded HIPSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |