Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1100-20 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-20 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-30 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 3101-20 Polyester BMC Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 3200-15 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-15 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0020 cm/cm | 0.0015 - 0.0020 in/in | ASTM D955 |
PolyOne Edgetek® PS-20CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | ISO 294-4 |
Solvay Specialty Polymers Ixef® 2011 Polyarylamide (PARA), 42% Mineral Filler
(discontinued **) Ixef 2011 is a general purpose, 42% mineral reinforcedpolyarylamide which exhibits high strength and stiffness, low warpage, and outstanding surface gloss.- Black: Ixef 2011/9000- Custom ColorableFe.. |
|||
Linear Mold Shrinkage | 0.0015 cm/cm | 0.0015 in/in | ISO 2577 |
Menzolit Menzolit® SMC 0650 Unsaturated Polyester UP SMC 0650 Low pressure SMC for large panels when moulding force becomes critical. Specific moulding pressure < 20 bar. A Special molding procedure is necessary.Information Provided by Menzolit |
|||
Linear Mold Shrinkage | 0.0015 - 0.0020 cm/cm | 0.0015 - 0.0020 in/in | 0.125; ASTM D955 |
LTL Color Compounds ColorFast® NY2GF330 Nylon 66, 33% Glass-Filled 33% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Linear Mold Shrinkage | 0.0015 cm/cm | 0.0015 in/in | ISO 2577 |
Sumitomo Bakelite North America RX® 630 Fiberglass Reinforced Phenolic RX 630 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North America. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | ASTM D955 |
Teknor Apex Chemlon® 133 GVH Nylon 66, 30% Glass Fiber Reinforced Notes: Excellent for connectors and electrical parts; Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Linear Mold Shrinkage | 0.0015 - 0.0040 cm/cm | 0.0015 - 0.0040 in/in | ASTM D955 |
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Features: Compound offering rigidity and strength, especially at high service temperatures; Excellent for large area parts Processing Method: Injection Molding Forms: Pellets Automotive Specificatio.. |
|||
Linear Mold Shrinkage | 0.0015 cm/cm | 0.0015 in/in | post shrinkage (2h/90°C) |
Borealis Daplen™ ED117AE Polypropylene TPO Compound Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | ISO 2577 |
Polyram RamSter PE304G3 PET, 15% Glass Fiber 15% Glass fiber reinforced, heat stabilized and impact modified PET for injection molding application.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.0015 cm/cm | 0.0015 in/in | ASTM D955 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0015 cm/cm | 0.0015 in/in | ASTM D955 |
Lubrizol ESTALOC® 59200 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Compression Molding. ASTM D955 |
Sumitomo Bakelite North America FS-4 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |