Physical Properties | Metric | English | Comments |
---|---|---|---|
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil LD 117.03 Blown Overwrap Film Resin
(discontinued **) LD 117 resins are homopolymer film resins with good clarity and excellent stiffness. Film from LD 117 resins can be used in overwrap applications and push-through type packaging equipment. Film ma.. |
|||
Slip Level | 750 ppm | 750 ppm | Additive - Erucamide |
Borealis Himod™ FT7324 . LDPE for Film Himod FT7324 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Slip Level | 750 ppm | 750 ppm | Erucamide |
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of.. |
|||
Slip Level | 750 ppm | 750 ppm | |
Chevron Phillips MarFlex® 5335 Low Density Polyethylene, Blown Film This LDPE is tailored for blown film applications that require:Good processabilityLow coefficient of frictionGood openabilityGood sealabilityTypical blown film applications include:Institutional pac.. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil Exceed™ 2018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018EB is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films. Availability: Africa & Middl.. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil LD 105.BR Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil LD 143.26 High Clarity Packaging Film Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil LDPE LD 100BR Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil LDPE LD 104BR Low Density Polyethylene Resin Product Description: LD 104BR is an LDPE grade, which offers good optical properties combined with increased stiffness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antibloc.. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil LDPE LD 136.MN Low Density Polyethylene Resin Product Description: LD 136.MN is a homopolymer film resin with good clarity. The resin is suitable for processing on blown film equipmentAvailability: Latin America, North America and South America.. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil LDPE LD 143.26 Low Density Polyethylene Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi.. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil LDPE LD 362BR Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
Slip Level | 750 ppm | 750 ppm | |
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP) AFFINITY™ PL 1881G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal products.In.. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil Exceed™ 1018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018EB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018EB have outstanding tensile, impact, puncture resistance and low temperature properties. .. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil Exceed™ 2018EB Blown Film Resin
(discontinued **) Exceed 2018EB resin is an ethylene based polymer produced with metallocene single site catalysts using ExxonMobil Chemicals Exxpol® Technology. The higher melt index makes this polymer ideally sui.. |
|||
Slip Level | 750 ppm | 750 ppm | |
ExxonMobil Exceed™ 1018 EB Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |