Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.927 g/cc | 0.0335 lb/in³ | ExxonMobil Method |
ExxonMobil Exceed™ 1327CA Blown Film Resin
(discontinued **) Exceed 1327CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1327CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Chevron Phillips 1124 Liner Grade Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Good Impact Strength, Good Processability, Low Gels, Good Sealability, Medium Slip, High AntiblockApplications:Trash Bags and other LinersProcessing Condition.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Chevron Phillips 5554-D LDPE High Clarity, Medium Impact, Low Slip Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Excellent Clarity, Good Impact Strength, Good Sealability, Low SlipApplications:Food Packaging, Case Shrink Wrap, LaminationsProcessing Conditions: Extruder 6.. |
|||
Density | 0.927 - 1.97 g/cc | 0.0335 - 0.0711 lb/in³ | Average value: 1.20 g/cc Grade Count:4 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Wire/Cable Grade". Each property range of values reported is min.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-312 EVA Film Resin, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 4.6% vinyl acetate copolymer resin for films with good toughness. This resin's low melt index and comonomer content help produce films which exhi.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Designed to be blended with a suitable masterbatch .. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Huntsman PE1605 EVA Film Extrusion
(discontinued **) 6% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ASTM D1505 |
LyondellBasell Microthene® G MU76300 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ASTM D1501 |
LyondellBasell Petrothene® NA443023 Blown Low Density Polyethylene ApplicationsPETROTHENE NA 443 is a series of low density/EVA copolymer resins for high impact/high clarity packaging applications. NA 443 exhibits excellent processability and good balance of optic.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ASTM D1505 |
LyondellBasell Plexar® PX3243 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ASTM D1505 |
LyondellBasell Purell® PE3020D Low Density Polyethylene, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding Purell PE 3020 D is a low density polyethylene with high rigidity, good opticals and good chemical resistance. It is delivered in pellet form. Target markets are small blow molding including packagi.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ISO 1183 |
Borealis Himod™ FT6273 LDPE for Film Himod FT6273 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ASTM D792 |
DuPont Bynel® 4105 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Westlake EB169 Low Density Polyethylene Westlake EB169 is a low-density polyethylene with high stiffness designed for beverage shrink overwrap and towel/tissue packaging. It has good toughness and blends well with LLDPE resins.Application.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ASTM D1505 |
Westlake EBAC® SP1802 22.5% Ethylene Butyl Acrylate Copolymer Westlake EBAC® SP1802 is a 22.5% EBA copolymer designed for blown film, tie-layer, coextrusions and blending where flexibility and strength are important. SP1802 provides excellent elasticity and l.. |
|||
Density | 0.927 - 0.944 g/cc | 0.0335 - 0.0341 lb/in³ | Requirement |
Westlake Plastics Lennite® GUR1020 (Type I) Ultra-high Molecular Weight Polyethylene For Medical Applications Medical grade Lennite UHMWPE is produced from premium resins in accordance with ASTM specification F648 and International Standard ISO 5834-1 for surgical implants. Westlake Plastics' proprietary m.. |
|||
Density | 0.927 - 0.944 g/cc | 0.0335 - 0.0341 lb/in³ | Requirement |
Westlake Plastics Lennite® GUR1050 (Type II) Ultra-high Molecular Weight Polyethylene For Medical Applications Medical grade Lennite UHMWPE is produced from premium resins in accordance with ASTM specification F648 and International Standard ISO 5834-1 for surgical implants. Westlake Plastics' proprietary m.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ASTM D1505 |
UBE B028 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ISO 1183 |
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Film Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityExcellent tear strengthHigh puncture resistanceGood stiffnessExcellent heat sealing proper.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ASTM D792 |
Total Lumicene® mPE M 3410 EP HDPE Film Outstanding clarity and gloss; excellent bubble stability; excellent tear strength; high puncture resistance; good stiffness; excellent heat sealing properties; excellent compatibility with LDPE and.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ExxonMobil method |
ExxonMobil Enable™ 27-05HH Metallocene Polyethylene Resin Product Description: Enable 27-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ExxonMobil method |
ExxonMobil Exceed™ 1327ED Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327ED is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327ED is fully formula.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ExxonMobil method |
ExxonMobil Exceed™ 1327KD Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327KD is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327KD is fully formula.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Bynel® 21E781 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | |
Dow Primacor® 4311 Ethylene Acrylic Acid (EAA) PRIMACOR® 4311 polymer containing 3% comonomer 3 is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent adhesion to metallic, p.. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | |
BASF Lucalen® A 2920 M Ethylene/Acrylate Copolymer Used in the manufacture of economical composite films of Lucalen and PE-LD, and as a primer for aluminum steel composites.Data was collected by ISO methods and provided by BASF. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | |
BASF Lucalen® A 2920 M Q 225 Ethylene/Acrylate Copolymer Data was collected by ISO methods and provided by BASF. |
|||
Density | 0.927 g/cc | 0.0335 lb/in³ | |
BASF Lucalen® A 2910 M Ethylene/Acrylate Copolymer For coating metals such as aluminum and steel, and as a primer for composites of metal or paper with Lupolen. Contains an antioxidant.Data was collected by ISO methods and provided by BASF. |
|||
Density | 0.927 - 0.945 g/cc | 0.0335 - 0.0341 lb/in³ | Average value: 0.939 g/cc Grade Count:17 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Molding Grade". Each property range of values reported is minimum an.. |