Download PDF LyondellBasell Plexar® PX3243 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, such as EVA or EMA, polypropylene, polyamide (nylon), ethylene vinyl alcohol copolymers (EVOH), ionomer and other sealants, polyethylene terephthalate (PET) resins and copolymers, styrenic polymers, metal, paper and many others. Product grades tailored for blown and cast films, sheet and thermoforming, blow molding, extrusion coating and lamination, tubing, pipe, spray coating and other specialty applications are available in pellet form. Contact your Plexar sales and/or Equistar technical service representative for more information and specific recommendations for your application(s).Regulatory Status: PX3243 meets the requirements for the Food and Drug Administration regulation 21CFR 175.105 for adhesives. This regulation describes adhesives which may be safely used as components of articles intended for use in packaging, transporting or holding food in accordance with conditions outlined in that regulation. For an adhesive formulation to be used in compliance with Section 175.105, it must be used under conditions that prevent the material from becoming a component of food in more than insignificant, de minimis, amounts. For more information, please contact your Equistar product safety representative.Processing Techniques: A process melt temperature above 410°F (210°C) is recommended to ensure adhesion between adherents. More specific suggestions can be made only when equipment, process parameters and conditions of use are known. Contact your Equistar Plexar technical service representative for more information.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.927 g/cc
0.0335 lb/in³
ASTM D1505
Water Vapor Transmission 4.30 g/m²/day
0.277 g/100 in²/day
ASTM F372
Thickness 50.8 microns
2.00 mil
Melt Flow 4.5 g/10 min
4.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.8 MPa
1710 psi
ASTM D882
Film Tensile Strength at Yield, TD 13.8 MPa
2000 psi
ASTM D882
Film Elongation at Break, MD 780 %
780 %
ASTM D882
Film Elongation at Break, TD 840 %
840 %
ASTM D882
Film Elongation at Yield, MD 12 %
12 %
ASTM D882
Film Elongation at Yield, TD 9.0 %
9.0 %
ASTM D882
Elmendorf Tear Strength MD 69 g
69 g
ASTM D1922
Elmendorf Tear Strength TD 241 g
241 g
ASTM D1922
Film Tensile Strength at Break, MD 22.9 MPa
3320 psi
ASTM D882
Film Tensile Strength at Break, TD 2.10 MPa
305 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 103 °C
217 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature >= 210 °C
>= 410 °F
Blow-up Ratio (BUR) 2.0
2.0