Physical Properties Metric English Comments
Density 1.38 - 1.67 g/cc
0.0499 - 0.0603 lb/in³
Average value: 1.43 g/cc Grade Count:148
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Density 1.49 - 1.67 g/cc
0.0538 - 0.0603 lb/in³
Average value: 1.53 g/cc Grade Count:20
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E..
Density 1.02 - 1.67 g/cc
0.0368 - 0.0603 lb/in³
Average value: 1.20 g/cc Grade Count:126
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Density 1.41 - 1.67 g/cc
0.0509 - 0.0603 lb/in³
Average value: 1.50 g/cc Grade Count:104
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Density 1.63 - 1.67 g/cc
0.0589 - 0.0603 lb/in³
ISO 1183
Fainplast Compounds Hax™ HFC 0108/4 Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding, designed to meet BS 7846Information provided by Fainplast Compounds
Density 1.14 - 1.67 g/cc
0.0410 - 0.0603 lb/in³
Average value: 1.36 g/cc Grade Count:665
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..
Density 1.07 - 1.67 g/cc
0.0385 - 0.0603 lb/in³
Average value: 1.24 g/cc Grade Count:133
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Density 1.14 - 1.67 g/cc
0.0412 - 0.0603 lb/in³
Average value: 1.27 g/cc Grade Count:363
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..
Density 1.33 - 1.67 g/cc
0.0480 - 0.0603 lb/in³
Average value: 1.45 g/cc Grade Count:16
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu..
Copyright © lookpolymers.com All Rights Reserved