Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.45 - 1.55 g/cc | 0.0524 - 0.0560 lb/in³ | wet density (as supplied) |
Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications Insural® 85 MASTIC is an asbestos-free, durable and insulating refractory composition designed for the fabrication of launders and jointing, bedding and patching of precast refractory shapes.Advant.. |
|||
Density | 1.50 - 1.55 g/cc | 0.0542 - 0.0560 lb/in³ | Average value: 1.52 g/cc Grade Count:4 |
Overview of materials for PVC, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Density | 1.31 - 1.55 g/cc | 0.0473 - 0.0560 lb/in³ | Average value: 1.42 g/cc Grade Count:8 |
Overview of materials for Phenolic, Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values .. |
|||
Density | 1.09 - 1.55 g/cc | 0.0394 - 0.0560 lb/in³ | Average value: 1.28 g/cc Grade Count:34 |
Overview of materials for Nylon 612, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 520/1 Rigid PVC, Extrusion Electric pipes |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds RK 325/AM Rigid PVC, Extrusion Lead Free Profiles anti mould |
|||
Density | 1.45 - 1.55 g/cc | 0.0524 - 0.0560 lb/in³ | Apparent |
Gouda Vuurvast FI 25-15 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Density | 1.50 - 1.55 g/cc | 0.0542 - 0.0560 lb/in³ | 380NS Resin |
Lord Adhesives Fusor® 380NS / 383NS Epoxy Adhesive LORD Fusor® 380NS/383NS adhesive is a two-part, rapid-cure epoxy adhesive used to bond fiberglass reinforced plastics (FRP), sheet molded compounds (SMC) and metals.All information provided by Lo.. |
|||
Density | 1.40 - 1.55 g/cc | 0.0506 - 0.0560 lb/in³ | |
Solvay RHODAFAC® BN-936/S Surfactant Identification: SODIUM TRIETHANOLAMINE PHOSPHATE IN AQUEOUS SOLUTIONAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: Oil field. Scale inhibition.Information provided .. |
|||
Density | 1.52 - 1.55 g/cc | 0.0549 - 0.0560 lb/in³ | |
Chengdu Polyster RPM540B Flame Retardant Masterbatch RPM540B is a red phosphorus based additive flame retardant designed for PBT resins. It is halogen-free and has good flame retardant performance. Red pellet form. Used for electrical componentsInform.. |
|||
Density | 1.52 - 1.55 g/cc | 0.0549 - 0.0560 lb/in³ | |
Chengdu Polyster RPM650 Flame Retardant Masterbatch RPM650 is a red phosphorus based additive flame retardant designed foruse in polyethylene resins. It is halogen free and has good flame retardant performance. Red pellet form. Wire insulation, elect.. |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1183 |
Fainplast Compounds FKA 89 Flexible PVC, Flame Retardant Insulation Lead Free Power cables |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 90 Flexible PVC, Flame Retardant Sheathing Lead Free General purposes |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 018/9 Halogen Free PVC General purpose |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 4021/TC Halogen Free PVC Improved flame retardancy |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds HGKA 0183 Flexible PVC, Sheathing for High Temperatures Lead Free Sheathing high LOI |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds R 316 Rigid PVC, Extrusion Rolling shutters |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds R 316/AS Rigid PVC, Extrusion Antistatic profiles |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 121 Rigid PVC, Extrusion Electric pipes |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 90 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds R 212/C Rigid PVC, Extrusion Shutters and shiny profiles |
|||
Density | 1.52 - 1.55 g/cc | 0.0549 - 0.0560 lb/in³ | MIL-PRF-81733D |
3M AC-665 Class C-12 Aerospace Sealant 3M Aerospace Sealant AC-665 Class C are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros.. |
|||
Density | 1.52 - 1.55 g/cc | 0.0549 - 0.0560 lb/in³ | MIL-PRF-81733D |
3M AC-665 Class C-48 Aerospace Sealant 3M Aerospace Sealant AC-665 Class C are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros.. |
|||
Density | 1.45 - 1.55 g/cc | 0.0524 - 0.0560 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow .. |
|||
Density | 1.45 - 1.55 g/cc | 0.0524 - 0.0560 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Density | 1.45 - 1.55 g/cc | 0.0524 - 0.0560 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Density | 1.08 - 1.55 g/cc | 0.0390 - 0.0560 lb/in³ | Average value: 1.28 g/cc Grade Count:77 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 84 Flexible PVC, Lead Free Pipes and profiles |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds R 244 Rigid PVC, Extrusion Shutters high modulus low curving |
|||
Density | 1.13 - 1.55 g/cc | 0.0408 - 0.0560 lb/in³ | Average value: 1.31 g/cc Grade Count:7 |
Overview of materials for Polyphenylene Ether, Glass/Graphite Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Glass/Graphite Reinforced". Each property range of values reported is minimum and m.. |